SUREWELD WELDING ELECTRODES

ESAB EXPANDS SUREWELD STICK ELECTRODES LINE

ESAB has expanded its line of Sureweld brand Stick welding electrodes, including an expanded number of grades and packaged the 3/32- and 1/8-in. diameter electrodes in 1- and 5-lb. resealable plastic tubes. The Sureweld portfolio is perfect for welders who use smaller quantities of a particular electrode grade or who want to use factory-fresh electrodes when starting a new project.

Sureweld carbon steel electrodes grades include 7018, 
6010, 6011, 6013, 7014 and 7024; stainless steel grades
available include 308L, 309L, 316L and 312. These grades
are available in 5/32-in. diameter, 5-lb. packages as well.

For a limited time, you may receive a free sample of Sureweld
electrodes with purchase of a ESAB Rogue welding machine.
For details, click here

Sureweld Stick Welding Electrodes
PRODUCT POSITION CURRENT ARC PENETRATION APPLICATION DESCRIPTION
SW 7018
E7018
All DCEP,
AC
Medium Medium Best used with clean or prepared welding surface. Designed to produce X-ray quality welds.
  SW 6010
E6010
All DCEP Digging Deep Excellent arc control, deep penetration allowing
to weld through rust, scale, oil and dirt. Adapts
exceptionally well to vertical and overhead.
  SW 6011
E6011
All DCEP,
AC
Digging Deep Use when you are unable to prepare a welding
surface. Its deep penetration allows welds through rust, scale, oil and dirt. ABS approved.
  SW 6013
E6013
All DCEP,
DCEN,
AC
Soft Light Best used with clean or prepared welding surface. Excellent for low heat applications designed for
general purpose.
  SW 7014
E7014
All DCEP,
DCEN,
AC
Soft Light Best used with clean or prepared welding surface. Designed for high deposition and high electrode travel speed.
  SW 7024
E7024
Flat,
H-Fillet
DCEP,
DCEN,
AC
Soft Light High deposition electrode used in Ship structures, bridges, structural steels, machine bases, truck
fabrication, storage tanks an rolling stocks.
  SW 308L
E308L-16
All DCEP,
AC
Soft Light For joining 304 and 304L stainless steel.
  SW 309L
E309L-16
All DCEP,
AC
Soft Light For use on joining stainless to carbon steel.
  SW 316L
E316L-16
All DCEP,
AC
Soft Light For joining 316 and 316L stainless steel. Widely used for food grade materials.
  SW 312 Repair
E312-16
All DCEP,
AC
Soft Light All propose stainless electrode. For repair, surfacing and joining of hard to weld metals.
  SW 55 Cast
ENiFe-Cl-A
All DCEP,
AC
Soft Light Used to build up, surfacing or joining on worn cast iron parts not needing tight dimensional control
or machining.