CaB System 300S/300M

ESAB
CaB System 300S/300M

Flexible, Modular Column and Booms


Featured

ESAB offers a totally integrated solution including welding process, manipulator movement as well as control of third axis products like the ESAB roller beds or positioners

  • Modular design concept allows total customization using standard components
  • Large selection of available components to integrate for a custom solution:
  • A variety of welding heads for SAW but also GMAW and GTAW
  • A complete range of rectifiers, transformers and inverter based power sources
  • The welding process is controlled from ESAB PEK or a PLC system
  • ESAB flux feeding and recovery systems
  • Monitoring systems and cameras
  • Choose from stationary or mobile, rail-travelling carriage systems
  • A Column and Boom ranging from 3x3 to 5x5 meter working range as standard
  • Single or twin wire set-up with the A2 or A6 welding head
  • 30 kg wire spools


Specifications

Weights

Concrete Stand Total Weight 1550 kg (3417 lb)
Foot Plate Total Weight 350 kg (772 lb)
Rail Carriage Total Weight 1670 kg (3681 lb)
x
CaB System 300S/300M

Documents


Speeds and Capacities

Model 3m (10ft) 4m (13ft) 5m (16.5ft)
Lifting Speed 27.5 in./min
0.7 m/min
27.5 in./min
0.7 m/min
27.5 in./min
0.7 m/min
Permissible Loads on Boom, max one end 530 lb
240 kg
331 lb
150 kg
165 lb
75 kg
Permissible Loads on Boom, max total 660 lb
300 kg
485 lb
220 kg
331 lb
150 kg
Transport Speed Boom and Rail Carriage 79 in./min
2.0 m/min
79 in./min
2.0 m/min
79 in./min
2.0 m/min
Welding Speed, Boom 4-79 in./min
0.1-2.0 m/min
4-79 in./min
0.1-2.0 m/min
4-79 in./min
0.1-2.0 m/min
Welding Speed, Rail Carriage 4-79 in./min
0.1-2.0 m/min
4-79 in./min
0.1-2.0 m/min
4-79 in./min
0.1-2.0 m/min

Weights

Concrete Stand Total Weight 1550 kg (3417 lb)
Foot Plate Total Weight 350 kg (772 lb)
Rail Carriage Total Weight 1670 kg (3681 lb)

Extra Information

Standard CaB Sizes
The manipulators are divided into three different sizes 300, 460 and 600. These sizes are the throat

dimensions of the boom in millimeters. Each size has a corresponding column. The different sizes are not

only limited in where it can fit, but also how far the boom can extend and how much load that can be put on.

Performance Categories
The system is divided into three different categories for performance:

S: Standard

Standard mechanical performance, no cable chain

A few options, camera-system, tacho-regulated speed and flux control

Only for Basic station 1

M: Modular

Standard mechanical performance, including cable chain for Columns and Booms

More than 20 options fully integrated, such as tandem, shift function, transport speed etc

Only for Basic station 1

C: Customized

Based on the same mechanical performance as the S- and M- model

Based on the same electrical system as the M- model

Includes everything that is not a S- or M- model such as:

Basic station 2, 3, and 4

Odd sizes (ex. 4.35 m x 5.15 m)

Option demands not offered in S- or M- model.

x

Interested in this product? Contact us.

Contact us online

Call our Product Information & Support Line anytime: 1-800-ESAB-123 (1-800-372-2123)

Welding & Cutting Equipment
181 East Evans Street Suite 18
Florence, SC 29506
Phone: (843)-669-4411

Cutting Systems
181 East Evans Street Suite 18
Florence, SC 29506
Phone: (843)-664-4394

Welding Consumables
801 Wilson Avenue
Hanover, PA 17331
Phone:(717)-637-8911
Fax: (717)-637-9859

Colfax Corporation
420 National Business Parkway
5th Floor
Annapolis Junction, MD 20701


x
×

Find the Closest Distributor

x

x

Loading..