A-Series Power Supply

ESAB

A-Series Power Supply

The following items have been added to your list


x

The A-Series systems are based on an industrial proven platform. The A-Series offers standard features to meet the needs of many automated applications. With all the advantages of 1Torch and proven systems reliability, the automated A-Series delivers the best in productivity, precision and performance.

BUY NOW


Features

  • All units have 80% duty cycle
  • Single phase 208/230V available on all units
  • Superior cut quality up to 120A
  • Lightweight and compact design
  • Durable in the toughest environments


Industries

  • Pipe Construction
  • Transportation
  • Power Poles
  • General Manufacturing
  • HVAC

Dimensions

Model A40i/A60i A80/A120
Dimensions 536 mm (21.1 in.) x 199 mm (7.8 in.) x 359 mm (14.1 in.) 660 mm (30 in.) x 248 mm (9.7 in.) x 343 mm (13.5 in.)

Cutting Specifications

Model A120 A40i A60i A80
Recommended Cut 6 mm (1/4 in.) 10 mm (3/8 in.) 12 mm (1/2 in.) 15 mm (5/8 in.)
Maximum Cut 12 mm (1/2 in.) 15 mm (5/8 in.) 20 mm (3/4 in.) 20 mm (3/4 in.)
Maximum Edge Start 25 mm (1 in.) 25 mm (1 in.) 30 mm (1 1/4 in.) 40 mm (1 1/2 in.)

Operating Specifications

Model A40i/A60i A80/A120
Enclosure Class IP23C
IP23C
Open Circuit VDC High 300 VDC
260 VDC

Weight

Description or Qualifier A40i/A60i A80/A120
Weight 15.9 kg (35 lb) 28.6 kg (63 lb)

Input Ratings

Frequency Hz 50/60 Hz
Phase 3

Output Ratings

Model A120 A40i A60i A80
Duty Cycle 100 %
80 %
80 %
100 %
100 %
80 %
100 %
80 %
Output Current DC 30-120 A
100 A
120 A
40 A
30 A
10-40 A
50 A
60 A
10-60 A
30-100 A
70 A
80 A
Output Power 15.4 kW
4.8 kW
7.9 kW
12 kW

Plasma Gas Requirements

Model All Models
Gas Pressure 5.2 bar (75.4 psig)
Gas Flow 189 l/min (400.5 cfh)