Type 318MP One Piece Gouging Propylene Tip

Victor

Type 318MP One Piece Gouging Propylene Tip

The following items have been added to your list


x

Propylene Cutting Tips - Type 318MP for gouging and rivet washing

BUY NOW


Features

  • General purpose
  • Propylene gouging and rivet washing


Industries

  • Industrial and General Fabrication
  • Structural Steel Fabrication
  • Repair and Maintenance
  • Light Fabrication
Type 318MP One Piece Gouging Propylene Tip

Documents


Fuel Specifications

Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Fuel Gas 5-9 psig
Part Number 0330-0333
Total Fuel Gas Consumption 14-18 cfh
Total Oxygen Consumption 150-175 cfh
Total Preheat Oxygen Consumption (imp) 23-108 cfh
Gas Pressure - Cutting Oxygen 45-50 psig
Gas Pressure - Fuel Gas 6-10 psig
Part Number 0330-0333
Total Fuel Gas Consumption 14-18 cfh
Total Oxygen Consumption 175-200 cfh
Total Preheat Oxygen Consumption (imp) 23-108 cfh
Gas Pressure - Cutting Oxygen 45-50 psig
Gas Pressure - Fuel Gas 8-12 psig
Part Number 0330-0335
Total Fuel Gas Consumption 16-20 cfh
Total Oxygen Consumption 210-250 cfh
Total Preheat Oxygen Consumption (imp) 23-108 cfh
Gas Pressure - Cutting Oxygen 45-55 psig
Gas Pressure - Fuel Gas 10-15 psig
Part Number 0330-0336
Total Fuel Gas Consumption 25-35 cfh
Total Oxygen Consumption 400-500 cfh
Total Preheat Oxygen Consumption (imp) 23-153 cfh
Gas Pressure - Cutting Oxygen 55-65 psig
Gas Pressure - Fuel Gas 10-15 psig
Part Number 0330-0336
Total Fuel Gas Consumption 25-35 cfh
Total Oxygen Consumption 450-500 cfh
Total Preheat Oxygen Consumption (imp) 23-153 cfh

Operating Specifications

Average Kerf Width 0.10 in.
Cutting Speed 10-14 in./min
Metal Thickness 2 in.
Part Number 0330-0333
Tip Size 3 in.
Average Kerf Width 0.10 in.
Cutting Speed 9-12 in./min
Metal Thickness 2 1/2 in.
Part Number 0330-0333
Tip Size 3 in.
Average Kerf Width 0.12 in.
Cutting Speed 8-11 in./min
Metal Thickness 3 in.
Part Number 0330-0335
Tip Size 4 in.
Average Kerf Width 0.17 in.
Cutting Speed 5-7 in./min
Metal Thickness 6 in.
Part Number 0330-0336
Tip Size 6 in.
Average Kerf Width 0.18 in.
Cutting Speed 4-6 in./min
Metal Thickness 8 in.
Part Number 0330-0336
Tip Size 6 in.
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Type 318MP One Piece Gouging Propylene Tip
Victor Professional Cutting Tip, Type 318MP, Size: 3 0330-0333 FIND A DISTRIBUTOR
Victor Professional Cutting Tip, Type 318MP, Size: 4 0330-0335 FIND A DISTRIBUTOR
Victor Professional Cutting Tip, Type 318MP, Size: 6 0330-0336 FIND A DISTRIBUTOR
x
x

x

Loading..