OXWELD 1520 Series'

ESAB

OXWELD 1520 Series

OXWELD 1520 Series

For gouging, grooving plate edges for welding, removing defects from castings, pad washing.

BUY NOW


Featured

  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • Precise CNC controlled drilling process ensures consistency in performance and quality
  • One-piece tips have triple swaged interior – gas passages are mirror smooth with internal
  • angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Long, parallel preheat passages permit re-dressing tips without affecting performance
  • One-piece tips are a single piece of solid copper– provide maximum cooling – recommended always for acetylene, and for other fuel gases when heat exposure is unusually severe
  • Two-piece tips – recommended for high efficiency with alternate fuels – solid copper, heavy-wall external sleeve and brass internal sections can be ordered separately to minimize replacement cost

Industries

  • Industrial and General Fabrication
  • Repair and Maintenance
  • Structural Steel Fabrication
  • Light Fabrication

Specifications

Fuel Specifications

08Z67

Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 30-35 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Total Acetylene Consumption 6-8 cfh
Total Oxygen Consumption 35-45 cfh

15Z17

Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Total Acetylene Consumption 8-10 cfh
Total Oxygen Consumption 65-75 cfh

Operating Specifications

15X33

Tip Size 13 in. (330 mm)

15X34

Tip Size 19 in. (483 mm)

Tip Specifications

Cleaning Drill Size Cutting 55
Cleaning Drill Size Preheat 56
Tip Size 13 in. (330 mm)
Cleaning Drill Size Cutting 49
Cleaning Drill Size Preheat 55
Tip Size 19 in. (483 mm)
x

Fuel Specifications

08Z67

Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 30-35 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Total Acetylene Consumption 6-8 cfh
Total Oxygen Consumption 35-45 cfh

15Z17

Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Total Acetylene Consumption 8-10 cfh
Total Oxygen Consumption 65-75 cfh

15Z18

Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Total Acetylene Consumption 14-16 cfh
Total Oxygen Consumption 120-135 cfh

15Z19

Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Total Acetylene Consumption 14-16 cfh
Total Oxygen Consumption 130-140 cfh
Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Total Acetylene Consumption 16-20 cfh
Total Oxygen Consumption 150-170 cfh
Gas Pressure - Acetylene 6-8 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Total Acetylene Consumption 16-20 cfh
Total Oxygen Consumption 185-210 cfh
Gas Pressure - Acetylene 6-8 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 20-30 psig
Total Acetylene Consumption 16-20 cfh
Total Oxygen Consumption 190-235 cfh
Gas Pressure - Acetylene 6-8 psig
Gas Pressure - Cutting Oxygen 45-60 psig
Gas Pressure - Preheat Oxygen 20-30 psig
Total Acetylene Consumption 16-20 cfh
Total Oxygen Consumption 205-255 cfh
Gas Pressure - Acetylene 6-8 psig
Gas Pressure - Cutting Oxygen 50-55 psig
Gas Pressure - Preheat Oxygen 25-30 psig
Total Acetylene Consumption 19-22 cfh
Total Oxygen Consumption 235-285 cfh

15Z20

Gas Pressure - Acetylene 8-10 psig
Gas Pressure - Cutting Oxygen 35-45 psig
Gas Pressure - Preheat Oxygen 25-30 psig
Total Acetylene Consumption 20-25 cfh
Total Oxygen Consumption 395-460 cfh
Gas Pressure - Acetylene 8-10 psig
Gas Pressure - Cutting Oxygen 55-65 psig
Gas Pressure - Preheat Oxygen 30-35 psig
Total Acetylene Consumption 30-35 cfh
Total Oxygen Consumption 545-625 cfh

15Z21

Gas Pressure - Acetylene 8-10 psig
Gas Pressure - Cutting Oxygen 65-75 psig
Gas Pressure - Preheat Oxygen 30-35 psig
Total Acetylene Consumption 40-45 cfh
Total Oxygen Consumption 630-710 cfh
Gas Pressure - Acetylene 10-12 psig
Gas Pressure - Cutting Oxygen 55-65 psig
Gas Pressure - Preheat Oxygen 30-35 psig
Total Acetylene Consumption 45-55 cfh
Total Oxygen Consumption 790-905 cfh

13A97

Gas Pressure - Acetylene 11-13 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 35-40 psig
Total Acetylene Consumption 75-80 cfh
Total Oxygen Consumption 1,300-1,695 cfh

13A98

Gas Pressure - Acetylene 11-13 psig
Gas Pressure - Cutting Oxygen 45-75 psig
Gas Pressure - Preheat Oxygen 40-60 psig
Total Acetylene Consumption 80-90 cfh
Total Oxygen Consumption 1,600-1,900 cfh

Operating Specifications

15X33

Tip Size 13 in. (330 mm)

15X34

Tip Size 19 in. (483 mm)

Tip Specifications

Cleaning Drill Size Cutting 55
Cleaning Drill Size Preheat 56
Tip Size 13 in. (330 mm)
Cleaning Drill Size Cutting 49
Cleaning Drill Size Preheat 55
Tip Size 19 in. (483 mm)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OXWELD 1520 Series
Series 1520 Tip, 19 inch, Propane Natural Gas 15X34 FIND A DISTRIBUTOR
Series 1520 Tip, 13 inch, Propane Natural Gas 15X33 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..