  • Deseaming, scarfing, gouging
  • Rivet washing
  • Weld preparation


Industries

  • Industrial and General Fabrication
  • Structural Steel Fabrication
  • Repair and Maintenance
  • Light Fabrication
Type 118 Acetylene Gouging Tip

Documents


Fuel Specifications

Gas Pressure - Acetylene 3-6 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 4-9 psig
Part Number 0330-0113
Total Acetylene Consumption 10-16 cfh
Total Oxygen Consumption 140-150 cfh
Total Preheat Oxygen Consumption 11-18 cfh
Gas Pressure - Acetylene 3-7 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 4-12 psig
Part Number 0330-0113
Total Acetylene Consumption 12-18 cfh
Total Oxygen Consumption 150-160 cfh
Total Preheat Oxygen Consumption 13-20 cfh
Gas Pressure - Acetylene 5-10 psig
Gas Pressure - Cutting Oxygen 40-50 psig
Gas Pressure - Preheat Oxygen 6-17 psig
Part Number 0330-0114
Total Acetylene Consumption 18-30 cfh
Total Oxygen Consumption 270-320 cfh
Total Preheat Oxygen Consumption 20-33 cfh
Gas Pressure - Acetylene 7-13 psig
Gas Pressure - Cutting Oxygen 45-40 psig
Gas Pressure - Preheat Oxygen 10-22 psig
Part Number 0330-0115
Total Acetylene Consumption 30-44 cfh
Total Oxygen Consumption 500-600 cfh
Total Preheat Oxygen Consumption 33-48 cfh
Gas Pressure - Acetylene 7-14 psig
Gas Pressure - Cutting Oxygen 45-55 psig
Gas Pressure - Preheat Oxygen 10-25 psig
Part Number 0330-0115
Total Acetylene Consumption 34-50 cfh
Total Oxygen Consumption 500-600 cfh
Total Preheat Oxygen Consumption 37-55 cfh
Gas Pressure - Acetylene 3-6 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 4-9 psig
Part Number 0331-0035
Total Acetylene Consumption 10-16 cfh
Total Oxygen Consumption 140-150 cfh
Total Preheat Oxygen Consumption 11-18 cfh
Gas Pressure - Acetylene 3-7 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 4-12 psig
Part Number 0331-0035
Total Acetylene Consumption 12-18 cfh
Total Oxygen Consumption 150-160 cfh
Total Preheat Oxygen Consumption 13-20 cfh

Operating Specifications

Average Kerf Width .09 in.
Cutting Speed 15-19 in./min
Metal Thickness 1 in.
Part Number 0330-0113
Tip Size 2 in.
Average Kerf Width .09 in.
Cutting Speed 13-17 in./min
Metal Thickness 1 1/2 in.
Part Number 0330-0113
Tip Size 2 in.
Average Kerf Width .12 in.
Cutting Speed 9-12 in./min
Metal Thickness 3 in.
Part Number 0330-0114
Tip Size 4 in.
Average Kerf Width .18 in.
Cutting Speed 6-8 in./min
Metal Thickness 6 in.
Part Number 0330-0115
Tip Size 6 in.
Average Kerf Width .19 in.
Cutting Speed 5-6 in./min
Metal Thickness 8 in.
Part Number 0330-0115
Tip Size 6 in.
Average Kerf Width .09 in.
Cutting Speed 15-19 in./min
Metal Thickness 1 in.
Part Number 0331-0035
Tip Size 2 in.
Average Kerf Width .09 in.
Cutting Speed 13-17 in./min
Metal Thickness 1 1/2 in.
Part Number 0331-0035
Tip Size 2 in.
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Type 118 Acetylene Gouging Tip
Victor Professional Cutting Tip, Series 1, Type 118, 2, Acetylene 0330-0113
Victor Professional Cutting Tip, Type 118 (Round), Size: 2 0331-0035 FIND A DISTRIBUTOR
Victor Professional Cutting Tip, Type 118, Size: 4 0330-0114
Victor Professional Cutting Tip, Type 118, Size: 6 0330-0115 FIND A DISTRIBUTOR
x
x

x

Loading..