Acetylene Cutting Tips - Type 112 for bulk & rivet head applications

BUY NOW


Features

  • For cutting close to bulk heads
  • Also for the hand cutting of rivet heads


Industries

  • Industrial and General Fabrication
  • Structural Steel Fabrication
  • Repair and Maintenance
  • Light Fabrication
Type 112 Bulk Head Acetylene Tip

Documents


Fuel Specifications

Gas Pressure - Acetylene 3-6 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 4-9 psig
Part Number 0330-0086
Total Acetylene Consumption 10-16 cfh
Total Oxygen Consumption 140-150 cfh
Total Preheat Oxygen Consumption 11-18 cfh
Gas Pressure - Acetylene 3-7 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 4-12 psig
Part Number 0330-0086
Total Acetylene Consumption 12-18 cfh
Total Oxygen Consumption 150-160 cfh
Total Preheat Oxygen Consumption 13-20 cfh

Operating Specifications

Average Kerf Width .09 in.
Cutting Speed 15-19 in./min
Metal Thickness 1 in.
Part Number 0330-0086
Tip Size 2 in.
Average Kerf Width .09 in.
Cutting Speed 13-17 in./min
Metal Thickness 1 1/2 in.
Part Number 0330-0086
Tip Size 2 in.
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Type 112 Bulk Head Acetylene Tip
Victor Professional Cutting Tip, Type 108, Size: 2 0330-0086 FIND A DISTRIBUTOR
x
x

x

Loading..