Tyle 101-30 Acetylene Cutting Tips

Victor

Tyle 101-30 Acetylene Cutting Tips

The following items have been added to your list


x

Acetylene Cutting Tips - Type 101-30 for manual or mechanized applications with a 30 degree bend

BUY NOW


Features

  • General purpose
  • Hand and machine torch cutting 30°, with torch perpendicular


Industries

  • Industrial and General Fabrication
  • Structural Steel Fabrication
  • Repair and Maintenance
  • Light Fabrication
Tyle 101-30 Acetylene Cutting Tips

Documents


Fuel Specifications

Gas Pressure - Acetylene 3-5 psig
Gas Pressure - Cutting Oxygen 25-30 psig
Gas Pressure - Preheat Oxygen 3-5 psig
Part Number 0330-0198
Total Acetylene Consumption 5-8 cfh
Total Oxygen Consumption 55-60 cfh
Total Preheat Oxygen Consumption 5-9 cfh
Gas Pressure - Acetylene 3-5 psig
Gas Pressure - Cutting Oxygen 30-35 psig
Gas Pressure - Preheat Oxygen 3-6 psig
Part Number 0330-0198
Total Acetylene Consumption 6-10 cfh
Total Oxygen Consumption 60-65 cfh
Total Preheat Oxygen Consumption 7-11 cfh
Gas Pressure - Acetylene 3-5 psig
Gas Pressure - Cutting Oxygen 30-35 psig
Gas Pressure - Preheat Oxygen 4-7 psig
Part Number 0330-0199
Total Acetylene Consumption 8-13 cfh
Total Oxygen Consumption 80-85 cfh
Total Preheat Oxygen Consumption 9-14 cfh
Gas Pressure - Acetylene 3-6 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 4-9 psig
Part Number 0330-0284
Total Acetylene Consumption 10-16 cfh
Total Oxygen Consumption 140-150 cfh
Total Preheat Oxygen Consumption 11-18 cfh

Operating Specifications

Average Kerf Width .06 in.
Cutting Speed 24-28 in./min
Metal Thickness 3/8 in.
Part Number 0330-0198
Tip Size 0 in.
Average Kerf Width .06 in.
Cutting Speed 20-24 in./min
Metal Thickness 1/2 in.
Part Number 0330-0198
Tip Size 0 in.
Average Kerf Width .07 in.
Cutting Speed 17-21 in./min
Metal Thickness 3/4 in.
Part Number 0330-0199
Tip Size 1 in.
Average Kerf Width .09 in.
Cutting Speed 15-19 in./min
Metal Thickness 1 in.
Part Number 0330-0284
Tip Size 2 in.
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Tyle 101-30 Acetylene Cutting Tips
Victor Professional Cutting Tip, Type 101 - 30 Degree, Size: 0 0330-0198 FIND A DISTRIBUTOR
Victor Professional Cutting Tip, Type 101 - 30 Degree, Size: 1 0330-0199 FIND A DISTRIBUTOR
Victor Professional Cutting Tip, Type 101 - 30 Degree, Size: 2 0330-0284 FIND A DISTRIBUTOR
x
x

x

Loading..