OXWELD 1510 Series

ESAB

OXWELD 1510 Series

The following items have been added to your list


x

For riser removal. Except in length, comparable to 1502. Supplied straight, with instructions for bending.

BUY NOW


Features

  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • Precise CNC controlled drilling process ensures consistency in performance and quality
  • One-piece tips have triple swaged interior – gas passages are mirror smooth with internal
  • angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Long, parallel preheat passages permit re-dressing tips without affecting performance
  • One-piece tips are a single piece of solid copper– provide maximum cooling – recommended always for acetylene, and for other fuel gases when heat exposure is unusually severe
  • Two-piece tips – recommended for high efficiency with alternate fuels – solid copper, heavy-wall external sleeve and brass internal sections can be ordered separately to minimize replacement cost

Industries

  • Industrial and General Fabrication
  • Structural Steel Fabrication
  • Repair and Maintenance
  • Light Fabrication

Fuel Specifications

Gas Pressure - Acetylene 6-8 psig
Gas Pressure - Cutting Oxygen 25-30 psig
Gas Pressure - Preheat Oxygen 15-25 psig
Part Number 08Z40
Total Acetylene Consumption 16-20 cfh
Total Oxygen Consumption 185-210 cfh
Gas Pressure - Acetylene 6-8 psig
Gas Pressure - Cutting Oxygen 30-40 psig
Gas Pressure - Preheat Oxygen 15-25 psig
Part Number 08Z40
Total Acetylene Consumption 16-20 cfh
Total Oxygen Consumption 205-255 cfh
Gas Pressure - Acetylene 6-8 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 15-25 psig
Part Number 08Z40
Total Acetylene Consumption 19-22 cfh
Total Oxygen Consumption 235-285 cfh
Gas Pressure - Acetylene 6-10 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 20-30 psig
Part Number 08Z41
Total Acetylene Consumption 20-25 cfh
Total Oxygen Consumption 395-460 cfh
Gas Pressure - Acetylene 6-10 psig
Gas Pressure - Cutting Oxygen 55-65 psig
Gas Pressure - Preheat Oxygen 20-30 psig
Part Number 08Z41
Total Acetylene Consumption 30-35 cfh
Total Oxygen Consumption 545-625 cfh
Gas Pressure - Acetylene 6-10 psig
Gas Pressure - Cutting Oxygen 40-55 psig
Gas Pressure - Preheat Oxygen 20-30 psig
Part Number 08Z42
Total Acetylene Consumption 40-55 cfh
Total Oxygen Consumption 630-710 cfh
Gas Pressure - Acetylene 10-12 psig
Gas Pressure - Cutting Oxygen 55-65 psig
Gas Pressure - Preheat Oxygen 20-30 psig
Part Number 08Z42
Total Acetylene Consumption 45-55 cfh
Total Oxygen Consumption 790-905 cfh

Operating Specifications

Average Kerf Width .095 in.
Metal Thickness 2 in.
Part Number 08Z40
Tip Size 8 in.
Average Kerf Width .100 in.
Metal Thickness 3 in.
Part Number 08Z40
Tip Size 8 in.
Average Kerf Width .105 in.
Metal Thickness 4 in.
Part Number 08Z40
Tip Size 8 in.
Average Kerf Width .157 in.
Metal Thickness 6 in.
Part Number 08Z41
Tip Size 10 in.
Average Kerf Width .170 in.
Metal Thickness 8 in.
Part Number 08Z41
Tip Size 10 in.
Average Kerf Width 190 in.
Metal Thickness 10 in.
Part Number 08Z42
Tip Size 12 in.
Average Kerf Width .210 in.
Metal Thickness 12 in.
Part Number 08Z42
Tip Size 12 in.

Tip Specifications

Cleaning Drill Size Cutting 76
Preheat Holes 12
Tip Size 8 in.
Cleaning Drill Size Cutting 68
Preheat Holes 12
Tip Size 10 in.
Cleaning Drill Size Cutting 46
Preheat Holes 6
Tip Size 12 in.
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OXWELD 1510 Series
1510 NOZZLE #10 08Z41 FIND A DISTRIBUTOR
1510 NOZZLE #12 08Z42 FIND A DISTRIBUTOR
1510 NOZZLE #8 08Z40 FIND A DISTRIBUTOR
x
x

x

Loading..