General Purpose. Medium Preheat, sufficient preheat for cutting dirty plate and for beveling.

BUY NOW


Features

  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • One-piece nozzle has triple swaged interior – gas passages are mirror smooth with internal angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • One-piece nozzle has triple swaged interior – gas passages are mirror smooth with internal angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Long, parallel preheat passages – permit re-dressing nozzle without affecting performance
  • One-piece nozzle is a single piece of solid copper – provides maximum cooling – recommended always for acetylene, and for other fuel gases when heat exposure is unusually severe
  • Two-piece nozzles – recommended for high efficiency with fuel gases other than acetylene – solid copper, heavy-wall external sleeve and brass internal sections can be ordered separately to minimize replacement cost
  • Conical seats – instant aligning provides tight seal, prevents leaks around nozzle nut

Industries

  • Industrial and General Fabrication
  • Structural Steel Fabrication
  • Repair and Maintenance
  • Light Fabrication

Fuel Specifications

Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 30-35 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Part Number 08Z67
Total Acetylene Consumption 6-8 cfh
Total Oxygen Consumption 35-45 cfh
Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Part Number 15Z17
Total Acetylene Consumption 8-10 cfh
Total Oxygen Consumption 65-75 cfh
Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Part Number 15Z18
Total Acetylene Consumption 14-16 cfh
Total Oxygen Consumption 120-135 cfh
Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Part Number 15Z19
Total Acetylene Consumption 14-16 cfh
Total Oxygen Consumption 130-140 cfh
Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Part Number 15Z19
Total Acetylene Consumption 16-20 cfh
Total Oxygen Consumption 150-170 cfh
Gas Pressure - Acetylene 6-8 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Part Number 15Z19
Total Acetylene Consumption 16-20 cfh
Total Oxygen Consumption 185-210 cfh
Gas Pressure - Acetylene 6-8 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 20-30 psig
Part Number 15Z19
Total Acetylene Consumption 16-20 cfh
Total Oxygen Consumption 190-235 cfh
Gas Pressure - Acetylene 6-8 psig
Gas Pressure - Cutting Oxygen 45-60 psig
Gas Pressure - Preheat Oxygen 20-30 psig
Part Number 15Z19
Total Acetylene Consumption 16-20 cfh
Total Oxygen Consumption 205-255 cfh
Gas Pressure - Acetylene 6-8 psig
Gas Pressure - Cutting Oxygen 50-55 psig
Gas Pressure - Preheat Oxygen 25-30 psig
Part Number 15Z19
Total Acetylene Consumption 19-22 cfh
Total Oxygen Consumption 235-285 cfh
Gas Pressure - Acetylene 8-10 psig
Gas Pressure - Cutting Oxygen 35-45 psig
Gas Pressure - Preheat Oxygen 25-30 psig
Part Number 15Z20
Total Acetylene Consumption 20-25 cfh
Total Oxygen Consumption 395-460 cfh
Gas Pressure - Acetylene 8-10 psig
Gas Pressure - Cutting Oxygen 55-65 psig
Gas Pressure - Preheat Oxygen 30-35 psig
Part Number 15Z20
Total Acetylene Consumption 30-35 cfh
Total Oxygen Consumption 545-625 cfh
Gas Pressure - Acetylene 8-10 psig
Gas Pressure - Cutting Oxygen 65-75 psig
Gas Pressure - Preheat Oxygen 30-35 psig
Part Number 15Z21
Total Acetylene Consumption 40-45 cfh
Total Oxygen Consumption 630-710 cfh
Gas Pressure - Acetylene 10-12 psig
Gas Pressure - Cutting Oxygen 55-65 psig
Gas Pressure - Preheat Oxygen 30-35 psig
Part Number 15Z21
Total Acetylene Consumption 45-55 cfh
Total Oxygen Consumption 790-905 cfh
Gas Pressure - Acetylene 11-13 psig
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Preheat Oxygen 35-40 psig
Part Number 13A97
Total Acetylene Consumption 75-80 cfh
Total Oxygen Consumption 1,300-1,695 cfh
Gas Pressure - Acetylene 11-13 psig
Gas Pressure - Cutting Oxygen 45-75 psig
Gas Pressure - Preheat Oxygen 40-60 psig
Part Number 13A98
Total Acetylene Consumption 80-90 cfh
Total Oxygen Consumption 1,600-1,900 cfh

Operating Specifications

Average Kerf Width .045 in.
Cutting Speed 17-25 in./min
Metal Thickness 1/4 in.
Part Number 08Z67
Tip Size 1/4 in.
Average Kerf Width .065 in.
Cutting Speed 15-23 in./min
Metal Thickness 1/2 in.
Part Number 15Z17
Tip Size 1/2 in.
Average Kerf Width .075 in.
Cutting Speed 13-21 in./min
Metal Thickness 3/4 in.
Part Number 15Z18
Tip Size 1-1/2 in.
Average Kerf Width .080 in.
Cutting Speed 12-18 in./min
Metal Thickness 1 in.
Part Number 15Z19
Tip Size 1-1/2 in.
Average Kerf Width .090 in.
Cutting Speed 11-16 in./min
Metal Thickness 1-1/2 in.
Part Number 15Z19
Tip Size 1-1/2 in.
Average Kerf Width .095 in.
Cutting Speed 10-14 in./min
Metal Thickness 2 in.
Part Number 15Z19
Tip Size 4 in.
Average Kerf Width .095 in.
Cutting Speed 9-12 in./min
Metal Thickness 2-1/2 in.
Part Number 15Z19
Tip Size 4 in.
Average Kerf Width .100 in.
Cutting Speed 8-11 in./min
Metal Thickness 3 in.
Part Number 15Z19
Tip Size 4 in.
Average Kerf Width .015 in.
Cutting Speed 6-9 in./min
Metal Thickness 4 in.
Part Number 15Z19
Tip Size 4 in.
Average Kerf Width .157 in.
Cutting Speed 4.5-6.5 in./min
Metal Thickness 6 in.
Part Number 15Z20
Tip Size 8 in.
Average Kerf Width .170 in.
Cutting Speed 3.5-5.0 in./min
Metal Thickness 8 in.
Part Number 15Z20
Tip Size 8 in.
Average Kerf Width .190 in.
Cutting Speed 2.9-3.8 in./min
Metal Thickness 10 in.
Part Number 15Z21
Tip Size 12 in.
Average Kerf Width .210 in.
Cutting Speed 2.4-3.0 in./min
Metal Thickness 12 in.
Part Number 15Z21
Tip Size 12 in.
Average Kerf Width .320 in.
Cutting Speed 3.0-3.5 in./min
Metal Thickness 18 in.
Part Number 13A97
Tip Size 18 in.
Average Kerf Width .360 in.
Cutting Speed 2-3 in./min
Metal Thickness 20 in.
Part Number 13A98
Tip Size 20 in.

Tip Specifications

Cleaning Drill Size Cutting 68
Cleaning Drill Size Preheat 69
Metal Thickness 1/4 in.
Preheat Holes 6
Tip Size 1/4 in.
Cleaning Drill Size Cutting 60
Cleaning Drill Size Preheat 66
Metal Thickness 1/2 in.
Preheat Holes 6
Tip Size 1/2 in.
Cleaning Drill Size Cutting 53
Cleaning Drill Size Preheat 65
Metal Thickness 1-1/2 in.
Preheat Holes 6
Tip Size 1-1/2 in.
Cleaning Drill Size Cutting 46
Cleaning Drill Size Preheat 61
Metal Thickness 2-4 in.
Preheat Holes 6
Tip Size 4 in.
Cleaning Drill Size Cutting 39
Cleaning Drill Size Preheat 57
Metal Thickness 6-8 in.
Preheat Holes 6
Tip Size 8 in.
Cleaning Drill Size Cutting 31
Cleaning Drill Size Preheat 56
Metal Thickness 9-12 in.
Preheat Holes 6
Tip Size 12 in.
Cleaning Drill Size Cutting 15
Cleaning Drill Size Preheat 54
Metal Thickness 16-18 in.
Preheat Holes 6
Tip Size 18 in.
Cleaning Drill Size Cutting 8
Cleaning Drill Size Preheat 54
Metal Thickness 20 in.
Preheat Holes 6
Tip Size 20 in.

Extra Info

1502 Series not recommended for acetylene pressure less than 5 psig.
***Sizes 16, 18, 20 recommended for use only with C-37 and C-39 torch.

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OXWELD 1502 Series
1502 NOZZLE 1 1/2 IN 15Z18 FIND A DISTRIBUTOR
1502 NOZZLE 1/2 IN 15Z17 FIND A DISTRIBUTOR
1502 NOZZLE 1/4 IN 08Z67 FIND A DISTRIBUTOR
1502 NOZZLE 12 IN 15Z21 FIND A DISTRIBUTOR
1502 NOZZLE 4 IN 15Z19 FIND A DISTRIBUTOR
1502 NOZZLE 8 IN 15Z20 FIND A DISTRIBUTOR
x
x

x

Loading..