PL Series Self Lighting Tips

TurboTorch

PL Series Self Lighting Tips

PL Series Self Lighting Tips

Increase the range of your torch kit with additional self lighting tips. All TurboTorch® tips feature an orifice screw that can be easily removed for simple cleaning or replacement, extending the life of the tip. All TurboTorch® tips feature an orifice screw that can be easily removed for simple cleaning or replacement, extending the life of the tip.

BUY NOW


Featured

  • All TurboTorch® tips feature an orifice screw that can be easily removed for simple cleaning or replacement, extending the life of the tip.

Industries

  • Hobbyist
  • HVAC
  • Light Fabrication

Specifications

Fuel Specifications

PL-3A

Gas Pressure - Acetylene 0.9 bar (14 psi)
Total Acetylene Consumption 3.6 cfh (0.108 cmh)

PL-5A

Gas Pressure - Acetylene 0.9 bar (14 psi)
Total Acetylene Consumption 5 cfh (0.15 cmh)

Operating Specifications

PL-3A

BTU per hour 1280
Silver Solder 1/8-1/2 in. (3-12 mm)
Soft Solder 1/4-1 in. (10-25 mm)
Tip Size 3/16 in. (5.0 mm)

PL-5A

BTU per hour 2080
Silver Solder 1/4-3/4 in. (10-20 mm)
Soft Solder 3/4-1 1/2 in. (20-40 mm)
Tip Size 1/4 in. (6.4 mm)
x
PL Series Self Lighting Tips

Fuel Specifications

PL-3A

Gas Pressure - Acetylene 0.9 bar (14 psi)
Total Acetylene Consumption 3.6 cfh (0.108 cmh)

PL-5A

Gas Pressure - Acetylene 0.9 bar (14 psi)
Total Acetylene Consumption 5 cfh (0.15 cmh)

PL-8A

Gas Pressure - Acetylene 0.9 bar (14 psi)
Total Acetylene Consumption 7 cfh (0.21 cmh)

PL-12A

Gas Pressure - Acetylene 0.9 bar (14 psi)
Total Acetylene Consumption 9 cfh (0.27 cmh)

Gas Replacement Parts

Model Orifice Part Number Tip
PL-12A OR-T-6 0386-0820 12A-TE
PL-3A OR-A3 0386-0874 3A-TE
PL-5A OR-A8 0386-0818 5A-TE
PL-8A 0386-0819 8A-TE

Operating Specifications

PL-3A

BTU per hour 1280
Silver Solder 1/8-1/2 in. (3-12 mm)
Soft Solder 1/4-1 in. (10-25 mm)
Tip Size 3/16 in. (5.0 mm)

PL-5A

BTU per hour 2080
Silver Solder 1/4-3/4 in. (10-20 mm)
Soft Solder 3/4-1 1/2 in. (20-40 mm)
Tip Size 1/4 in. (6.4 mm)

PL-8A

BTU per hour 2520
Silver Solder 1/2-1 in. (15-30 mm)
Soft Solder 1-2 in. (25-50 mm)
Tip Size 5/16 in. (7.9 mm)

PL-12A

BTU per hour 3360
Silver Solder 1-2 in. (25-50 mm)
Soft Solder 2-4 in. (50-90 mm)
Tip Size 3/8 in. (9.5 mm)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : PL Series Self Lighting Tips
PL-5A Tip Swirl, Air Acetylene, Self Lighting 0386-0818 FIND A DISTRIBUTOR
PL-8A Tip Swirl, Air Acetylene, Self Lighting 0386-0819 FIND A DISTRIBUTOR
PL-12A Tip Swirl, Air Acetylene, Self Lighting 0386-0820 FIND A DISTRIBUTOR
PL-3A Tip Swirl, Air Acetylene, Self Lighting 0386-0874 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..