OK Tigrod 410NiMo
Bare welding rods of the 420NiMo type alloyed with 13% Cr, 4.5% Ni and 0.5% Mo. This alloy is used for welding similar composition martensitic and martensitic-ferritic steels in different applications, such as hydroturbines.
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Cu | Mn | Mo | Ni | Si | ||||||||
0.02 % | 12.4 % | 0.1 % | 0.5 % | 0.6 % | 4.2 % | 0.4 % |
Typical Charpy V-Notch Properties
Classifications
Name | EN ISO 14343-A |
Grade | W 13 4 |
2 |
Consumable Characteristics
Alloy Type | Martensitic-ferritic (13 % Cr - 4.5 % Ni - 0.5 % Mo) |
Typical Tensile Properties
Stress relieved | Stress relieved | |
Tensile Strength (met) | 1000 MPa(145 ksi) | 870 MPa(126 ksi) |
Yield Strength (met) | 930 MPa(135 ksi) | 770 MPa(112 ksi) |
Elongation | 17 % | 22 % |
Testing Time | 2 hr | 8 hr |
Testing Temperature (met) | 600 degC(1112 degF) | 600 degC(1112 degF) |