Bare, corrosion-resistant, chromium-nickel rods for welding stabilised austenitic chromium-nickel alloys of the 18% Cr-8% Ni type. The rods are stabilised with niobium, which provides good resistance to the intergranular corrosion of the weld metal. Due to the niobium content, this alloy is recommended for use at higher temperatures.

BUY NOW


Typical Weld Metal Analysis %

Wire Composition
C Cr Cu Mn Mo Nb Ni Si Si+Fe
0.04 % 19.3 % 0.05 % 1.4 % 0.10 % 0.50 % 9.5 % 0.4 % 7 %

Approvals

Society NAKS/HAKC
Grade 2.4mm
Approvals are based on factory location. Please contact ESAB for more information.

Typical Charpy V-Notch Properties

Testing Temperature 20 degC
Testing Temperature 68 degF
Impact Value (met) 130 J
Impact Value (imp) 96 ft-lb
Conditional Statement As welded

Classifications

Grade ~1.4551
Name Werkstoffnummer
Grade ER347
Name SFA/AWS A5.9
Grade W 19 9 Nb
Name EN ISO 14343-A

Consumable Characteristics

Alloy Type Austenitic (with approx. 8 % ferrite) 19% Cr - 9% Ni - Nb

Typical Tensile Properties

ElongationTensile Strength (imp)Yield Strength (imp)
35 %655 MPa (95 ksi)510 MPa (74 ksi)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Tigrod 347
OK TIGROD 347 1/16X39X11#CT 162116R150 FIND A DISTRIBUTOR
OK Tigrod 347 2.0x1000mm 5kg 162120R150 FIND A DISTRIBUTOR
TIGROD 347 3/32X39X5KG CJ 162124R150 FIND A DISTRIBUTOR
TIGROD 347 1/8X39X5KG CJ 162132R150 FIND A DISTRIBUTOR
x
x

x

Loading..