Bare, corrosion-resistant, stabilised, chromium-nickel-molybdenum wire for welding Cr-Ni-Mo and Cr-Ni stabilised or non-stabilised steels. OK Tigrod 318Si has good general corrosion resistance. The alloy is stabilised with niobium to improve resistance to the intergranular corrosion of the weld metal. The higher silicon content improves the welding properties such as wetting. Due to stabiliation by niobium, this alloy is recommended for service temperatures up to 400°C.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
70 J (52 ft-lb) -60 degC (-76 degF)
40 J (29.5 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded35 %615 MPa (89 ksi)460 MPa (67 ksi)

Deposition Data

Diameter
3.2 mm
2.4 mm
2 mm
4 mm
1.6 mm
1.2 mm
1 mm

Classifications

Wire Electrode Werkstoffnummer : ~1.4576
EN ISO 14343-A : W 19 12 3 Nb Si
SFA/AWS A5.9 : ER318 (mod)

Approvals

Approvals CE EN 13479
DB 43.039.15
NAKS/HAKC 2.0 mm
VdTÜV 09737
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic (with approx. 7 % ferrite) 19% Cr - 12% Ni - 3 % Mo - Nb

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Mn Mo Nb Ni P S Si
0.04 % 19 % 0.1 % 1.3 % 2.8 % 0.5 % 12 % 0.02 % 0.01 % 0.8 %
Typical Wire Composition %
0.05 % 18.8 % 0.10 % 1.7 % 2.60 % 0.50 % 11.9 % - - 0.8 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Tigrod 318Si
163110R150 FIND A DISTRIBUTOR
163112R150 FIND A DISTRIBUTOR
163116R150 FIND A DISTRIBUTOR
163120R150 FIND A DISTRIBUTOR
163124R150 FIND A DISTRIBUTOR
163132R150 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..