OK Tigrod 317L
Bare, corrosion-resistant, chromium-nickel-molybdenum welding rods for welding austenitic stainless alloys of the 19% Cr, 9% Ni, 3% Mo types. OK Tigrod 317L has good resistance to general corrosion and pitting due to its high content of molybdenum. The alloy has a low carbon content which makes it particularly recommended when there is a risk of intergranular corrosion. The alloy is used in severe corrosion conditions such as in the petrochemical, pulp and paper industries.
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | FN WRC-92 | Mn | Mo | N | Ni | Si | |||||||
0.01 % | 18.9 % | 7 % | 1.4 % | 3.6 % | 0.05 % | 13.6 % | 0.4 % |