Bare, corrosion-resistant, chromium-nickel welding rod for welding heat-resistant austenitic steels of the 25Cr-20Ni type. The wire has a high Cr content and provides good oxidation resistance at high temperatures. Common applications include industrial furnaces and boiler parts, as well as heat exchangers.
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Cu | Mn | Mo | Ni | Si | ||||||||
0.10 % | 25.8 % | 0.05 % | 1.6 % | 0.10 % | 20.7 % | 0.4 % |