OK Tigrod 309MoL

ESAB

OK Tigrod 309MoL

The following items have been added to your list


x

Bare, corrosion-resistant rod of “309LMo’’ type. OK Tigrod 309MoL is used for the overlay welding of unalloyed and low-alloyed steels and for welding dissimilar steels such as 316L to unalloyed and low-alloyed steels when Mo is essential.

BUY NOW


Typical Weld Metal Analysis %

Wire Composition
C Cr Mn Mo Ni Si
0.01 % 21.4 % 1.5 % 2.5 % 14.6 % 0.4 %

Approvals

Society DNV-GL
Grade VL 309 MoL (I1)
Approvals are based on factory location. Please contact ESAB for more information.

Typical Charpy V-Notch Properties

Classifications

Grade ER309LMo (mod)
Name SFA/AWS A5.9
Grade W 23 12 2 L
Name EN ISO 14343-A

Consumable Characteristics

Alloy Type Austenitic (with approx. 8% ferrite) "309LMo", 22 % Cr - 15 % Ni - 3 % Mo - Low C

Typical Tensile Properties

ElongationTensile Strength (imp)Yield Strength (imp)
30 %610 MPa (88.5 ksi)500 MPa (72.5 ksi)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Tigrod 309MoL
OK Tigrod 309MoL 1.6x500mm 1kg 165416R51C FIND A DISTRIBUTOR
OK Tigrod 309MoL 2.0x1000 5kg 165420R150 FIND A DISTRIBUTOR
OK Tigrod 309MoL 2.0x500mm 1kg 165420R51C FIND A DISTRIBUTOR
OK Tigrod 309MoL 2.4x1000 5kg 165424R150 FIND A DISTRIBUTOR
OK Tigrod 309MoL 2.4x500mm 1kg 165424R51C FIND A DISTRIBUTOR
x