OK Tigrod 309L
Bare corrosion resisting chromium-nickel welding rod for welding of similar steels of 24% Cr, 13% Ni types. The alloy is also used for welding of buffer layers on CMn steels and welding of dissimilar joints. When using the wire for buffer layers and dissimilar joints it is necessary to control the dilution of the weld. OK Tigrod 309L has a good general corrosion resistance. When used for joining dissimilar materials the corrosion resistance is of secondary importance.
Typical Charpy V-Notch Properties
Impact Value | Testing Temperature | |||
as welded | ||||
160 J (118 ft-lb) | 20 degC (68 degF) | |||
130 J (96 ft-lb) | -60 degC (-76 degF) | |||
90 J (66 ft-lb) | -110 degC (-166 degF) |
Typical Tensile Properties
Condition | Elongation | Tensile Strength | Yield Strength |
As Welded | 40 % | 590 MPa | 430 MPa |
Classifications
Wire Electrode |
Werkstoffnummer : ~1.4332 SFA/AWS A5.9 : ER309L EN ISO 14343-A : W 23 12 L |
Approvals
Grade | EN 13479 |
Society | CE |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | Austenitic (with approx. 10 % ferrite) 24 % Cr - 13 % Ni - Low C |
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | FN WRC-92 | Mn | Mo | N | Ni | Si | |||||||
0.02 % | 23.2 % | 10 % | 1.8 % | 0.10 % | 0.05 % | 13.4 % | 0.4 % |