OK Tigrod 308LSi
Bare, corrosion-resistant, chromium-nickel rods for welding austenitic chromium-nickel alloys of the18% Cr-8% Ni type. OK Tigrod 308LSi has good general corrosion resistance. The alloy has a low carbon content which makes it particularly recommended when there is a risk of intergranular corrosion. The higher silicon content improves the welding properties such as wetting. The alloy is widely used in the chemical and food-processing industries, as well as for pipes, tubes and boilers.
Typical Charpy V-Notch Properties
Impact Value | Testing Temperature | |||
as welded | ||||
150 J (111 ft-lb) | -60 degC (-76 degF) | |||
170 J (125 ft-lb) | 20 degC (68 degF) | |||
140 J (103 ft-lb) | -110 degC (-166 degF) | |||
75 J (55 ft-lb) | -196 degC (-321 degF) |
Typical Tensile Properties
Condition | Elongation | Tensile Strength | Yield Strength |
As Welded | 37 % | 625 MPa | 480 MPa |
Classifications
Wire Electrode |
SFA/AWS A5.9 : ER308LSi Werkstoffnummer : ~1.4316 EN ISO 14343-A : W 19 9 L Si |
Approvals
Grade | 308L BT |
Society | BV |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | Austenitic (with approx. 8 % ferrite) 19% Cr - 9% Ni - Low C |
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Cu | Mn | Mo | Ni | Si | Si+Fe | |||||||
0.01 % | 19.9 % | 0.10 % | 1.8 % | 0.15 % | 10.5 % | 0.9 % | 9 % |