OK Tigrod 308H

The following items have been added to your list


x

Bare, corrosion-resistant, chromium-nickel rods for welding austenic chromium-nickel alloys of the18% Cr-8% Ni type. OK Tigrod 308H has good general corrosion resistance. The alloy has a high carbon content, which makes it suitable for applications at higher temperatures. The alloy is used in the chemical and petrochemical industries for the welding of tubes, cyclones and boilers.

BUY NOW


Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded30 %550 MPa (80 ksi)350 MPa (51 ksi)

Classifications

Wire Electrode SFA/AWS A5.9 : ER308H
EN ISO 14343-A : W 19 9 H

Approvals

Grade 2.4mm
Society NAKS/HAKC
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic 19% Cr - 9% Ni - High C

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Mn Ni Si
0.05 % 19.8 % 1.9 % 9.2 % 0.5 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Tigrod 308H
161524R150 FIND A DISTRIBUTOR
161520R150 FIND A DISTRIBUTOR