Bare, corrosion-resistant, duplex welding rods for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo types. OK Tigrod 2209 has high general corrosion resistance. In media containing chloride and hydrogen sulphide, the alloy has high resistance to intergranular corrosion, pitting and especially to stress corrosion. The alloy is used in a variety of applications across all industrial segments.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
-10 degC (14 degF)
85 J (63 ft-lb) -20 degC (-76 degF)
60 J (44 ft-lb) -60 degC (-76 degF)
100 J (74 ft-lb) 20 degC (68 degF)
sht 1050°c (1922°f) 0.5h
110 J (81 ft-lb) -20 degC (-4 degF)
90 J (66 ft-lb) -60 degC (-76 degF)
130 J (96 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

Condition As Welded SHT
1050°C 0.5h
Tensile Strength 765 MPa 730 MPa
Yield Strength 600 MPa 450 MPa
Elongation 28 % 34 %

Deposition Data

Diameter
3.2 mm
2.4 mm
2 mm
1.6 mm
1.2 mm

Classifications

Wire Electrode SFA/AWS A5.9 : ER2209
EN ISO 14343-A : W 22 9 3 N L

Approvals

Approvals CE EN 13479
DB 43.039.19
NAKS/HAKC 1.6-3.2 mm
Only for lot numbers starting with IT : VdTÜV 05519
Only for lot numbers starting with FP : VdTÜV 06282
VdTÜV 13010
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic-ferritic (22.5 % Cr - 8 % Ni - 3 % Mo - Low C)

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr FN WRC-92 Mn Mo N Ni PRE Si
0.01 % 22.7 % 55 % 1.5 % 3.2 % 0.17 % 8.5 % 35 % 0.5 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Tigrod 2209
168612R150 FIND A DISTRIBUTOR
168616R150 FIND A DISTRIBUTOR
168616R51C FIND A DISTRIBUTOR
168620R150 FIND A DISTRIBUTOR
168620R51C FIND A DISTRIBUTOR
168624R150 FIND A DISTRIBUTOR
168624R15Q FIND A DISTRIBUTOR
168624R51C FIND A DISTRIBUTOR