OK Tigrod NiCrMo-3
Bare corrosion and heat-resisting Ni-Cr-Mo rods for welding of high alloyed heat-resisting and corrosion resisting materials, 9%Ni-steels and similar steels with high notch toughness at low temperatures. Also for joining of dissimilar metals of the types mentioned. The weld metal has very good mechanical properties at high and low temperatures. Good resistance to pitting and stress corrosion.
Typical Tensile Properties
Condition | Elongation | Tensile Strength | Yield Strength |
As Welded | 40 % | 780 MPa | 550 MPa |
Classifications
Wire Electrode |
SFA/AWS A5.14 : ERNiCrMo-3 EN ISO 18274 : S Ni 6625 |
Approvals
Grade | For NV1.5Ni up to NV9Ni |
Society | DNV |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | Alloyed nickel (Ni + 22 % Cr + 9 % Mo - 3.5 % Nb) |
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Fe | Mn | Mo | Nb+Ta | Ni | Si | |||||||
0.02 % | 22.7 % | 0.3 % | 0.04 % | 8.6 % | 3.5 % | 64.8 % | 0.06 % |