OK Tigrod NiCr-3
Bare corrosion and heat-resisting Ni-Cr-Mo rods for welding of high alloyed heat-resisting and corrosion resisting materials, 9%Ni-steels and similar steels with high notch toughness at low temperatures. Also for joining of dissimilar metals of the types mentioned. The weld metal has very good mechanical properties at high and low temperatures. Good resistance to pitting and stress corrosion.
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Fe | Mn | Nb+Ta | Ni | Si | ||||||||
0.04 % | 20.0 % | 1.3 % | 3.0 % | 2.5 % | bal % | 0.2 % |
Approvals
Society | NAKS/HAKC |
Grade | 2.4 mm |
Approvals are based on factory location. Please contact ESAB for more information. |
Typical Charpy V-Notch Properties
Testing Temperature | 20 degC |
Testing Temperature | 68 degF |
Impact Value (met) | 150 J |
Impact Value (imp) | 111 ft-lb |
Conditional Statement | As welded |