OK Tigrod Ni-1
A bare nickel based rod alloyed with about 3% Ti for welding of high purity nickel (min 99.6 %Ni), ordinary wrought nickel and nickel with reduced C content. The weld metal can be used in a wide range of applications were the construction is working with corrosive media.
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
Al | C | Cu | Fe | Mn | Ni | Si | Ti | |||||||
0.06 % | 0.01 % | 0.01 % | 0.04 % | 0.4 % | 96 % | 0.5 % | 3.1 % |
Approvals
Society | VdTÜV |
Grade | 12659 |
Approvals are based on factory location. Please contact ESAB for more information. |
Typical Charpy V-Notch Properties
Testing Temperature | 20 degC |
Testing Temperature | 68 degF |
Conditional Statement | As welded |
Classifications
Grade | ERNi-1 |
Name | SFA/AWS A5.14 |
Grade | S Ni 2061 (NiTi3) |
Name | EN ISO 18274 |
Consumable Characteristics
Alloy Type | Nickel (Ni + 2.5 % Ti) |