TIGROD ER80S-B6

TIGROD ER80S-B6

Tigrod ER80S-B6 is a Chrome-Moly TIG rod for joining 5% Cr - 0.5% Mo steels such as ASTM A200-T5, A335-P5 and A387-Gr5. These non-copper-coated rods are primarily used to fabricate and repair power piping, pressure vessels, heat exchangers, and boilers used in the power generation industry. All ESAB ER80S-B6 Tigrod is embossed on both ends with the alloy identification. This grade of rod was previously classified as ER502.

Where To Buy


Industries

  • Process
  • Petrochemical

Welding Process

  • GTAW (TIG - Tungsten Inert Gas )

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 24 % 1350 °F 1 hr 95 ksi 82 ksi
Stress Relieved 26 % 1375 °F 1 hr 93 ksi 80 ksi

Typical Weld Metal Analysis %

wire composition
PMnX-FactorCuMoSCVSiNiCr
max 0.012 %0.40-0.70 %max 12 %max 0.20 %0.45-0.65 %max 0.025 %0.05-0.10 %max 0.03 %0.15-0.50 %max 0.3 %4.5-6.0 %
weld metal analysis
PMnX-FactorCuMoSCVSiNiCr
0.007 %0.50 %< 15 % - 0.50 %0.01 %0.08 % - 0.40 % - 5.80 %

Classifications: ASME SFA 5.28; AWS A5.28; ER80S-B6

x

Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 24 % 1350 °F 1 hr 95 ksi 82 ksi
Stress Relieved 26 % 1375 °F 1 hr 93 ksi 80 ksi

Typical Weld Metal Analysis %

wire composition
PMnX-FactorCuMoSCVSiNiCr
max 0.012 %0.40-0.70 %max 12 %max 0.20 %0.45-0.65 %max 0.025 %0.05-0.10 %max 0.03 %0.15-0.50 %max 0.3 %4.5-6.0 %
weld metal analysis
PMnX-FactorCuMoSCVSiNiCr
0.007 %0.50 %< 15 % - 0.50 %0.01 %0.08 % - 0.40 % - 5.80 %

Classifications: ASME SFA 5.28; AWS A5.28; ER80S-B6

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : TIGROD ER80S-B6
NCU80SB6 1/8X36X10#T/30#CT 152JF52 Buy Local
NCU80SB6 3/32X36X10#T/30#CT 152JF50 Buy Local
NCU80SB6 1/16X36X10#T/30#CT 152JF48 Buy Local
NCU80SB6 5/32X36X10#T/30#CT 152JF54 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..