OK Tigrod 5183 was developed to provide the highest strengths possible in the as welded condition of alloy AA 5083 and other similar high magnesium alloys. The more common OK Tigrod 5356 will typically fail to meet the as-welded tensile requirements of AA 5083. The alloy is typically utilised in marine and structural applications where high strengths, high fracture toughness for impact resistance and exposure to corrosive elements are important. The alloy is not recommended for elevated temperature applications due to its susceptibility to stress corrosion cracking. The alloy is non-heat treatable.

BUY NOW


Typical Charpy V-Notch Properties

As Welded
Impact Value 67 ft-lb
Impact Value 90 J
Testing Temperature 68 °F
Testing Temperature 20 °C

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded25 %290 MPa (42 ksi)140 MPa (20 ksi)

Classifications

Wire Electrode EN ISO 18273 : S Al 5183 (AlMg4,5Mn0,7(A))
JIS Z 3232 : A5183
SFA/AWS A5.10 : R5183

Approvals

Approvals ABS R 5183
CE EN 13479
CWB ER5183
DB 61.039.04
JIS JIS Z 3232
NAKS/HAKC 4.0mm
NAKS/HAKC 3.2MM
VdTÜV 04667
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type AlMgMn

Typical Weld Metal Analysis %

Typical Wire Composition %
Al Cr Cu Fe Mg Mn Si Ti Zn
94.200 % 0.08 % 0.01 % 0.13 % 4.9 % 0.65 % 0.04 % 0.100 % 0.01 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Tigrod 5183
181616R120 FIND A DISTRIBUTOR
181620R150 FIND A DISTRIBUTOR
181620R120 FIND A DISTRIBUTOR
181624R150 FIND A DISTRIBUTOR
181624R120 FIND A DISTRIBUTOR
181632R150 FIND A DISTRIBUTOR
181632R120 FIND A DISTRIBUTOR
181640R150 FIND A DISTRIBUTOR
181640R120 FIND A DISTRIBUTOR
181648R120 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..