ESAB

OK Autrod 385

The following items have been added to your list


x

A continous solid corrosion resisting chromium-nickel-molybdenum-copper wire for welding of austenitic stainless alloys of 20% Cr, 25% Ni, 5% Mo, 1,5% Cu, low C types. OK Autrod 385 weld metal has a good resistance to stress corrosion and intergranular corrosion and shows a very good resistance to attack in non-oxidizing acids. The resistance and crevice corrosion is better than for ordinary 18% Cr, 8% Ni, Mo steels. The alloy is widely used in many applications related to the process industry. OK Autrod 385 can be used in combination with OK Flux 10.93.

BUY NOW


Classifications

Wire Electrode SFA/AWS A5.9 : ER385
EN ISO 14343-A : S 20 25 5 Cu L

Approvals

Grade 12101
Society VdTÜV
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Fully austenitic (20 % Cr - 25 % Ni - 5 % Mo - 1.5 % Cu - Low C)

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Cu Mn Mo N Ni Si
0.01 % 20.0 % 1.5 % 1.7 % 4.4 % 0.05 % 25.0 % 0.4 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 385
1655240300 FIND A DISTRIBUTOR
1655320300 FIND A DISTRIBUTOR
1655323110 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..