OK Autrod 347

The following items have been added to your list


x

A continuous solid corrosion resisting chromium-nickel wire for the welding of austenitic chromium nickel alloys of the 18% Cr - 8% Ni type. OK Autrod 347 has a good general corrosion resistance. The alloy is stabilized with niobium to improve the resistance against intergranular corrosion of the weld metal. Due to the niobium content this alloy is recommended for use at higher temperatures. OK Autrod 347 can be used in combination with OK Flux 10.93.

BUY NOW


Classifications

Wire Electrode EN ISO 14343-A : S 19 9 Nb
SFA/AWS A5.9 : ER347

Approvals

Approvals CE EN 13479
DB 52.039.07
CZ : NAKS/HAKC 2.4, 3.2, 4.0 mm
VdTÜV 12101
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic (with approx. 10 % ferrite) 19% Cr - 9% Ni - Nb

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr FN WRC-92 Mn N Nb Ni Si
0.04 % 19.2 % 7 % 1.4 % 0.05 % 0.6 % 9.5 % 0.4 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 347
1621163110 FIND A DISTRIBUTOR
1621203110 FIND A DISTRIBUTOR
1621243110 FIND A DISTRIBUTOR
1621323110 FIND A DISTRIBUTOR
1621320400 FIND A DISTRIBUTOR
1621403110 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..