OK Autrod 318 is an extra low carbon, stainless wire for the submerged arc welding of corrosion-resistant steels of the 18Cr12Ni3Mo type, such as AlSi 316 and 316L or somewhat lower alloyed types. OK Autrod 318 can be used in combination with OK Flux 10.93.

BUY NOW


Classifications

Wire Electrode EN ISO 14343-A : S 19 12 3 Nb
SFA/AWS A5.9 : ER318

Approvals

Approvals CE EN 13479
DB 52.039.11
NAKS/HAKC 4.0mm
VdTÜV 12101
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr FN WRC-92 Mn Mo N Nb Ni Si
0.04 % 18.9 % 11 % 1.8 % 2.6 % 0.04 % 0.7 % 11.5 % 0.4 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 318
1641243110 FIND A DISTRIBUTOR
1641323110 FIND A DISTRIBUTOR
1641403110 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..