A continous solid corrosion resisting chromium-nickel-molybdenum wire for welding of austenitic manganese steels of 25% Cr, 22% Ni, 2% Mo types. OK Autrod 310MoL has a good resistance to pitting, intergranular corrosion and stress corrosion cracking. The alloy is used in acid rich environments, in the urea industry and in gas treatment plants. OK Autrod 310MoL can be used in combination with OK Flux 10.93.

BUY NOW


Typical Weld Metal Analysis %

Wire Composition
C Cr FN WRC-92 Mn Mo N Ni Si
0.01 % 25.0 % 0 % 4.5 % 2.0 % 0.14 % 22.0 % 0.1 %

Classifications

Name EN ISO 14343-A
Grade S 25 22 2 N L
2

Consumable Characteristics

Alloy Type Austenitic (25% Cr - 22% Ni - 2% Mo - nitrogen - low carbon)