OK Autrod 309L
A continuous solid corrosion resisting chromium-nickel wire for joining stainless steels to non-alloy or low-alloy steels as well as for welding austenitic stainless alloys of 24% Cr, 13% Ni types. OK Autrod 309L has a good general corrosion resistance. When used for joining dissimilar materials, the corrosion resistance is of secondary importance. OK Autrod 309L can be used in combination with OK Flux 10.93.
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | FN WRC-92 | Mn | Mo | N | Ni | Si | |||||||
0.02 % | 23.2 % | 10 % | 1.8 % | 0.10 % | 0.05 % | 13.4 % | 0.4 % |
Approvals
Society | CE |
Grade | EN 13479 |
Approvals are based on factory location. Please contact ESAB for more information. |
Classifications
Wire Electrode |
SFA/AWS A5.9 : ER309L EN ISO 14343-A : S 23 12 L |
Consumable Characteristics
Alloy Type | Austenitic (with approx. 12 % ferrite) 24 % Cr - 13 % Ni - Low C |