OK Autrod 308L SAW
A continuous, solid, corrosion-resistant, chromium-nickel wire. OK Autrod 308L has good general corrosion resistance. The alloy has a low carbon content which makes it particularly suitable for applications where there is a risk of intergranular corrosion. OK Autrod 308L is widely used in the chemical and food-processing industries, as well as for pipes, tubes and boilers and can be used in combination with OK Flux 10.93, OK Flux 10.94 or OK Flux 10.95.
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Mn | N | Ni | Si | |||||||||
0.02 % | 19.8 % | 1.9 % | 0.05 % | 9.8 % | 0.4 % |
Approvals
Society | CE |
Grade | EN 13479 |
Approvals are based on factory location. Please contact ESAB for more information. |
Classifications
Wire Electrode |
SFA/AWS A5.9 : ER308L EN ISO 14343-A : S 19 9 L |
Consumable Characteristics
Alloy Type | Austenitic (with approx. 10 % ferrite) 19% Cr - 9% Ni - Low C |