OK Autrod 2209

ESAB

OK Autrod 2209

The following items have been added to your list


x

A duplex austenitic-ferritic stainless welding strip designed for submerged arc cladding. It is used with OK Flux 10.05 to produce a 2209 duplex stainless steel type of weld deposit.

BUY NOW


Typical Weld Metal Analysis %

Wire Composition
C Cr Mn Mo N Ni Si
0.01 % 22.7 % 1.5 % 3.2 % 0.17 % 8.5 % 0.5 %

Approvals

Approvals CE EN 13479
CZ : NAKS/HAKC 3.2-4.0mm
Approvals are based on factory location. Please contact ESAB for more information.

Classifications

Wire Electrode SFA/AWS A5.9 : ER2209
EN ISO 14343-A : S 22 9 3 N L

Consumable Characteristics

Alloy Type Austenitic-ferritic (22.5 % Cr - 8 % Ni - 3 % Mo - Low C)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 2209
OK Autrod 2209 1.6 mm 15 kg 1686169820 FIND A DISTRIBUTOR
OK Autrod 2209 2.0mm 25kg 1686203150 FIND A DISTRIBUTOR
OK AUTROD 2209 3/32X55#CL 1686243150 FIND A DISTRIBUTOR
OK Autrod 2209 2.4mm 300kg 1686243400 FIND A DISTRIBUTOR
OK Autrod 2209 2.4mm 350kg 1686240600 FIND A DISTRIBUTOR
OK AUTROD 2209 1/8X55# CL 1686323150 FIND A DISTRIBUTOR
OK Autrod 2209 3.2mm 280kg 1686320400 FIND A DISTRIBUTOR
OK Autrod 2209 3.2mm 300kg 1686323400 FIND A DISTRIBUTOR
OK Autrod 2209 4.0mm 25kg 1686403150 FIND A DISTRIBUTOR
x
x

x

Loading..