OK Flux 10.94 is a basic chromium-alloying flux for the butt welding of stainless steels. OK Flux 10.94 is a suitable flux for welding stainless, high-alloyed CrNiMo steels like super-duplex stainless steels.

BUY NOW


Classifications

Grade S A AF 2 56 64 DC
Name EN ISO 14174

Consumable Characteristics

Alloy Transfer Chromium compensating
Basicity Index nom: 1.9
Density nom: 1.0 kg/dm3
Slag Type Fluoride basic CaF2-Al2O3-SiO2

Flux Consumption

Volts kg Flux / kg Wire DC+
26 V 0.5 kg
30 V 0.6 kg
34 V 0.8 kg
38 V 1.0 kg
Amps Dimensions Travel speed
580 A 4.0 mm 33 m/h

Classifications

Wire AWS/EN
OK Autrod 308L A5.9:ER308L/ 14343-A:S 19 9 L
OK Autrod 2509 A5.9:ER2594/ 14343-A:S 25 9 4 N L
OK Autrod 347 A5.9:ER347/ 14343-A:S 19 9 Nb

Approvals

Combined with Wire
*Selected production units only. Please contact ESAB for more information. Visit esab.com to download specific flux/wire combination fact sheets for more details.

Typical Mechanical Properties

Combined with Wire Condition Yield Strength Tensile Strength Charpy V-Notch Elongation
OK Autrod 2509 As Welded DC+ 625 MPa
(91 ksi)
830 MPa
(120 ksi)
90 J @ 20°C,
(67 ft-lb @ 68 °F)
50 J @ -60°C,
(37 ft-lb @ -76 °F)
28 %
OK Autrod 308L As Welded DC+ 400 MPa 560 MPa 85 J
70 J
60 J
40 %
OK Autrod 347 As Welded DC+ 455 MPa 620 MPa 100 J
70 J
50 J
30 J
38 %

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu FN WRC-92 Mn Mo N Nb Ni Si
OK Autrod 2509 Current: DC+, 420A, 27V
0.02 % 24.5 % - 54 % 0.4 % 3.5 % 0.15 % - 10.1 % 0.5 %
OK Autrod 308L DC+
0.02 % 20 % 0.1 % - 1.4 % 0.2 % - - 9.5 % 0.5 %
OK Autrod 347 DC+
0.04 % 19.6 % - - 1.0 % - - 0.5 % 9.6 % 0.5 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Flux 10.94
1094000000 FIND A DISTRIBUTOR
109400000Q FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..