Agglomerated aluminate-fluoride-basic flux for welding of 9% Ni steels and other high alloyed steels with Ni based wires. The flux is manganese adding, which reduces the risk of hot cracking. Good slag detachability and nice bead appearance.

BUY NOW


Specifications


Approvals

Society Wire
DNV OK Autrod NiCrMo-3 SAW
- OK Autrod NiCrMo-13
DNV OK Autrod NiCrMo-4

Classifications

AWS/EN Wire
A5.14:ERNiCrMo-3/ 18274:S Ni 6625 (NiCr22Mo9Nb) OK Autrod NiCrMo-3 SAW
A5.9:ER310/ 14343-A:S 25 20 OK Autrod 310
A5.14:ERNiCrMo-4/ 18274:S Ni 6276 (NiCr15Mo16Fe6W4) OK Autrod NiCrMo-4
A5.14:ERNiCr-3/ 18274:S Ni 6082 (NiCr20Mn3Nb) OK Autrod NiCr-3
A5.14:ERNiCrMo-13/ 18274:S Ni 6059 (NiCr23Mo16) OK Autrod NiCrMo-13

Flux Consumption

Amps Dimensions kg Flux / kg Wire DC+ Travel speed Volts
580 A 4.0 mm 0.5 kg 33 m/h 26 V
580 A 4.0 mm - 33 m/h 26 V
580 A 4.0 mm 0.6 kg 33 m/h 30 V
580 A 4.0 mm - 33 m/h 30 V
580 A 4.0 mm 0.8 kg 33 m/h 34 V
580 A 4.0 mm - 33 m/h 34 V
580 A 4.0 mm 1.0 kg 33 m/h 38 V
580 A 4.0 mm - 33 m/h 38 V

Typical Mechanical Properties

Charpy V-Notch Charpy V-Notch Testing Temp Condition Elongation Tensile Strength Wire Yield Strength
52 ft-lb -321 °F As Welded 46 % 98 ksi OK Autrod NiCrMo-13 68 ksi
74 ft-lb -321 °F As Welded 42 % 104 ksi OK Autrod NiCrMo-3 SAW 64 ksi
44 ft-lb -321 °F As Welded 35 % 101.5 ksi OK Autrod NiCrMo-4 70 ksi
107 ft-lb -112 °F As Welded 35 % 87 ksi OK Autrod NiCr-3 58 ksi
96 ft-lb -321 °F As Welded 35 % 87 ksi OK Autrod NiCr-3 58 ksi

Typical Weld Metal Analysis

chemical composition
SiO2+TiO2CaF2Al2O3+MnO
10 %45 %40 %

Approvals: NAKS/HAKC; RD 03-613-03
Classifications: EN ISO 14174; S A AF 2 55 53 MnNi DC

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Transfer: IMPERIAL_Chromium compensating. Nickel- and manganese alloying.
Basicity Index: nom: 1.7
Density: nom: 1.0 kg/dm3
Slag Type: Fluoride basic CaF2-Al2O3-SiO2
x

Approvals

Society Wire
DNV OK Autrod NiCrMo-3 SAW
- OK Autrod NiCrMo-13
DNV OK Autrod NiCrMo-4

Classifications

AWS/EN Wire
A5.14:ERNiCrMo-3/ 18274:S Ni 6625 (NiCr22Mo9Nb) OK Autrod NiCrMo-3 SAW
A5.9:ER310/ 14343-A:S 25 20 OK Autrod 310
A5.14:ERNiCrMo-4/ 18274:S Ni 6276 (NiCr15Mo16Fe6W4) OK Autrod NiCrMo-4
A5.14:ERNiCr-3/ 18274:S Ni 6082 (NiCr20Mn3Nb) OK Autrod NiCr-3
A5.14:ERNiCrMo-13/ 18274:S Ni 6059 (NiCr23Mo16) OK Autrod NiCrMo-13

Flux Consumption

Amps Dimensions kg Flux / kg Wire DC+ Travel speed Volts
580 A 4.0 mm 0.5 kg 33 m/h 26 V
580 A 4.0 mm - 33 m/h 26 V
580 A 4.0 mm 0.6 kg 33 m/h 30 V
580 A 4.0 mm - 33 m/h 30 V
580 A 4.0 mm 0.8 kg 33 m/h 34 V
580 A 4.0 mm - 33 m/h 34 V
580 A 4.0 mm 1.0 kg 33 m/h 38 V
580 A 4.0 mm - 33 m/h 38 V

Typical Mechanical Properties

Charpy V-Notch Charpy V-Notch Testing Temp Condition Elongation Tensile Strength Wire Yield Strength
52 ft-lb -321 °F As Welded 46 % 98 ksi OK Autrod NiCrMo-13 68 ksi
74 ft-lb -321 °F As Welded 42 % 104 ksi OK Autrod NiCrMo-3 SAW 64 ksi
44 ft-lb -321 °F As Welded 35 % 101.5 ksi OK Autrod NiCrMo-4 70 ksi
107 ft-lb -112 °F As Welded 35 % 87 ksi OK Autrod NiCr-3 58 ksi
96 ft-lb -321 °F As Welded 35 % 87 ksi OK Autrod NiCr-3 58 ksi

Typical Weld Metal Analysis

chemical composition
SiO2+TiO2CaF2Al2O3+MnO
10 %45 %40 %

Approvals: NAKS/HAKC; RD 03-613-03
Classifications: EN ISO 14174; S A AF 2 55 53 MnNi DC

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Transfer: IMPERIAL_Chromium compensating. Nickel- and manganese alloying.
Basicity Index: nom: 1.7
Density: nom: 1.0 kg/dm3
Slag Type: Fluoride basic CaF2-Al2O3-SiO2
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Flux 10.90
OK Flux 10.90 25kg 1090000000 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..