Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Fe | Mn | Mo | Nb+Ta | Ni | Si | |||||||
0.02 % | 22.7 % | 0.3 % | 0.04 % | 8.6 % | 3.5 % | bal % | 0.06 % |
Approvals
Society | NAKS/HAKC |
Grade | 2.4-3.2 mm |
Approvals are based on factory location. Please contact ESAB for more information. |
Classifications
Wire Electrode |
SFA/AWS A5.14 : ERNiCrMo-3 EN ISO 18274 : S Ni 6625 (NiCr22Mo9Nb) |
Consumable Characteristics
Alloy Type | NiCrMo-3 |