ESAB

OK Autrod NiCrMo-13

The following items have been added to your list


x

OK Autrod NiCrMo-13 is a Nb-free, Ni-Cr-Mo wire for welding high-alloyed steels of the 20Cr25Ni4-6Mo type and nickel-based alloys of similar type. The wire can also be used for welding these steels with dissimilar steels. The weld metal has very good corrosion resistance in both oxidizing and reducing media. OK Autrod NiCrMo-13 can be combined with OK Flux 10.90 or OK Flux 10.16.

BUY NOW


Classifications

Wire Electrode SFA/AWS A5.14 : ERNiCrMo-13
EN ISO 18274 : S Ni 6059 (NiCr23Mo16)

Typical Weld Metal Analysis %

Typical Wire Composition %
Al C Cr Fe Mn Mo Ni Si
0.3 % 0.01 % 23.0 % 1.0 % 0.2 % 16.0 % bal % 0.1 %