OK Autrod NiCr-3
OK Autrod NiCr-3 is a corrosion and heat resistant, nickel-chromium wire for submerged arc welding of high alloyed steel, heat resistant steel, corrosion resistant steel, 9Ni steels and similar steels with high notch toughness at low temperatures. OK Autrod NiCr-3 can be combined with OK Flux 10.90 or OK Flux 10.16.
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Fe | Mn | Nb+Ta | Ni | Si | ||||||||
0.04 % | 20.0 % | 1.3 % | 3.0 % | 2.5 % | bal % | 0.2 % |
Approvals
Society | NAKS/HAKC |
Grade | 3.2 mm |
Approvals are based on factory location. Please contact ESAB for more information. |
Classifications
Wire Electrode |
SFA/AWS A5.14 : ERNiCr-3 EN ISO 18274 : S Ni 6082 (NiCr20Mn3Nb) |