Agglomerated aluminate-fluoride-basic flux for welding of 9% Ni steels and other high alloyed steels with Ni based wires. The flux is manganese adding, which reduces the risk of hot cracking. Good slag detachability and nice bead appearance.

BUY NOW


Classifications

Grade S A AF 2 55 53 MnNi DC
Name EN ISO 14174

Approvals

Grade RD 03-613-03
Society NAKS/HAKC
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Transfer Chromium compensating. Nickel- and manganese alloying.
Basicity Index nom: 1.7
Density nom: 1.0 kg/dm3
Slag Type Fluoride basic CaF2-Al2O3-SiO2

Flux Consumption

Volts kg Flux / kg Wire DC+
26 V 0.5 kg
30 V 0.6 kg
34 V 0.8 kg
38 V 1.0 kg
Amps Dimensions Travel speed
580 A 4.0 mm 33 m/h

Classifications

Wire AWS/EN
OK Autrod NiCrMo-13 A5.14:ERNiCrMo-13/ 18274:S Ni 6059 (NiCr23Mo16)
OK Autrod NiCr-3 A5.14:ERNiCr-3/ 18274:S Ni 6082 (NiCr20Mn3Nb)
OK Autrod NiCrMo-3 SAW A5.14:ERNiCrMo-3/ 18274:S Ni 6625 (NiCr22Mo9Nb)
OK Autrod NiCrMo-4 A5.14:ERNiCrMo-4/ 18274:S Ni 6276 (NiCr15Mo16Fe6W4)
OK Autrod NiCrMo-3 A5.14:ERNiCrMo-3/ 18274:S Ni 6625 (NiCr22Mo9Nb)
OK Autrod 310 A5.9:ER310/ 14343-A:S 25 20

Approvals

Wire ABS DNV
OK Autrod NiCrMo-3 SAW - *
OK Autrod NiCrMo-4 * *
*Selected production units only. Please contact ESAB for more information. Visit esab.com to download specific flux/wire combination fact sheets for more details.

Typical Mechanical Properties

Wire Condition Yield Strength Tensile Strength Charpy V-Notch Elongation
OK Autrod 310 As Welded ISO DC+ 390 MPa 570 MPa 85 J 34 %
OK Autrod NiCr-3 As Welded ISO DC+ 400 MPa 600 MPa 145 J
130 J
35 %
OK Autrod NiCrMo-13 As Welded 350 A, HI 1.3-1.7 kJ/mm DC+ 470 MPa 675 MPa 70 J 46 %
OK Autrod NiCrMo-3 As Welded HI ~1.0-1.7 kJ/mm DC+ 440 MPa 720 MPa 100 J 42 %
OK Autrod NiCrMo-3 SAW As Welded HI ~1.0-1.7 kJ/mm DC+ 440 MPa 720 MPa 100 J 42 %
OK Autrod NiCrMo-4 As Welded DC+ 480 MPa 700 MPa 60 J 35 %

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Fe Mn Mo Nb+Ta Ni Si W
OK Autrod NiCr-3
0.004 % 19.3 % 1.7 % 4.4 % 0.1 % 2.6 % Bal % 0.35 % -
OK Autrod NiCrMo-13 Current Type: DC+ , 350A, 29V
0.01 % 22.0 % 1 % 2.8 % 15.0 % - bal. % 0.2 % -
OK Autrod NiCrMo-3 DC+, 350A, 29V
0.01 % 21.0 % 2.0 % 1.7 % 8.5 % 3.0 % Bal. % 0.2 % -
OK Autrod NiCrMo-4 DC+, 350A, 29V
0.01 % 15.0 % 6.0 % 2.2 % 15.5 % - Bal. % 0.2 % 3.4 %