OK Flux 10.16 is an agglomerated fluoride basic, non-alloying flux for submerged arc welding specially designed for joining as well as overlay applications on Ni-based alloys.

BUY NOW


Classifications

Grade S A FB 2 55 43 DC
Name EN ISO 14174

Approvals

Grade RD 03-613-03
Society NAKS/HAKC
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Transfer Moderately manganese and silicon alloying
Basicity Index nom: 2.4
Density nom: 1.2 kg/dm3
Slag Type Fluoride basic CaF2-Al2O3-(TiO2)-(MnO)
Welding Current 900 A (60 x 0.5 mm strip)

Classifications

Wire AWS/EN
OK Autrod NiCrMo-13 A5.14:ERNiCrMo-13/ 18274:S Ni 6059 (NiCr23Mo16)
OK Autrod NiCr-3 A5.14:ERNiCr-3/ 18274:S Ni 6082 (NiCr20Mn3Nb)
OK Autrod NiCrMo-3 SAW A5.14:ERNiCrMo-3/ 18274:S Ni 6625 (NiCr22Mo9Nb)
OK Autrod NiCrMo-3 A5.14:ERNiCrMo-3/ 18274:S Ni 6625 (NiCr22Mo9Nb)

Approvals

Combined with Wire VdTÜV
OK Band NiCr3 *
*Selected production units only. Please contact ESAB for more information. Visit esab.com to download specific flux/wire combination fact sheets for more details.

Typical Mechanical Properties

Combined with Wire Condition Yield Strength Tensile Strength Charpy V-Notch Elongation
OK Autrod NiCr-3 As Welded 325A DC+ Feed speed: 25m/h 360 MPa
(52 ksi)
600 MPa
(87 ksi)
140 J @ 20°C,
(104 ft-lb @ 68 °F)
100 J @ -196°C,
(74 ft-lb @ -320.8 °F)
41 %
OK Autrod NiCrMo-13 As Welded 300A DC+ Feed speed: 25m/h 490 MPa
(71 ksi)
730 MPa
(106 ksi)
80 J @ 20°C,
(59 ft-lb @ 68 °F)
75 J @ -60°C,
(56 ft-lb @ -76 °F)
60 J @ -196°C,
(44 ft-lb @ -320.8 °F)
44 %
OK Autrod NiCrMo-3 As Welded HI ~1.0-1.7 kJ/mm DC+ 450 MPa
(65 ksi)
720 MPa
(104 ksi)
100 J @ -140°C,
(74 ft-lb @ -220 °F)
90 J @ -196°C,
(67 ft-lb @ -320.8 °F)
43 %
OK Autrod NiCrMo-3 SAW As Welded HI ~1.0-1.7 kJ/mm DC+ 450 MPa 720 MPa 100 J
90 J
43 %

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
Al C Co Cr Cu Fe Mn Mo Nb+Ta Ni P S Si
OK Autrod NiCr-3 DC+ , 325A, 30V
- 0.01 % - 19.0 % - 1.3 % 3.2 % - 2.3 % Bal. % 0.010 % 0.010 % 0.3 %
OK Autrod NiCrMo-13 Current Type: DC+ , 300A, 30V
0.1 % 0.02 % 0.1 % 18.0 % - 2.0 % 0.7 % 16.5 % 0.1 % Bal % - - 0.2 %
OK Autrod NiCrMo-3 DC+, 320A, 30V
- 0.01 % - 19.5 % 0.08 % 2.0 % 0.6 % 8.5 % 3.0 % Bal. % 0.01 % 0.01 % 0.3 %
OK Band NiCr3 DC+, 750A, 28V, 12cm/min
- 0.02 % - 20.0 % - - 3.0 % - 2.5 % Bal % - - 0.5 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Flux 10.16
1016000000 FIND A DISTRIBUTOR
101600000Q FIND A DISTRIBUTOR
1016400000 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..