SPOOLARC 71'

ESAB

SPOOLARC 71

SPOOLARC 71

Spoolarc 71 is a medium manganese and silicon subarc wire that has been microalloyed with titanium. Used with 429, OK 10.62, and OK 10.71 fluxes Spoolarc 71 will produce weld deposits with a minimum 70,000 psi tensile strength in the as welded condition or after eight-hours of stress relief. When used with OK 10.62 weld deposits meet ASME A No. 1 chemistry requirements. Spoolarc 71 is used for welding pressure vessles and can be used for other applications requiring good mechanical properties after stress relieving.

BUY NOW


Industries

  • Pressure Vessels
  • Pipe Construction

Welding Process

  • SAW - Submerged Arc Welding

Specifications


Typical Weld Metal Analysis

wire composition
PMnCSTiSi
0.01 %1.22 %0.10 %0.01 %0.07 %0.55 %

Classifications: ASME SFA 5.17; AWS A5.17; EM14K

x

Typical Weld Metal Analysis

wire composition
PMnCSTiSi
0.01 %1.22 %0.10 %0.01 %0.07 %0.55 %

Classifications: ASME SFA 5.17; AWS A5.17; EM14K

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : SPOOLARC 71
71 5/64X65#CL 13L4F29 FIND A DISTRIBUTOR
71 3/32X65#CL 13L4F30 FIND A DISTRIBUTOR
71 1/8X65#CL 13L4F32 FIND A DISTRIBUTOR
71 5/32X65#CL 13L4F34 FIND A DISTRIBUTOR
71 3/16X65#CL 13L4F35 FIND A DISTRIBUTOR
71 3/32X1000#DR 13L6F90 FIND A DISTRIBUTOR
71 1/8X1000#DR 13L6F92 FIND A DISTRIBUTOR
71 5/32X1000#DR 13L6F94 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..