SPOOLARC 53

ESAB
SPOOLARC 53

Designed for single or multipass welding on carbon and low alloy steels. Provides higher strength deposits with moderate rust and mill scale tolerance. Produces good impact toughness. Applications include pressure vessel fabrication and offshore oil rig structures.

BUY NOW


Industries

  • Automotive
  • Agricultural Equipment
  • Mobile Equipment
  • Industrial and General Fabrication

Welding Process

  • SAW - Submerged Arc Welding

Specifications


Typical Weld Metal Analysis %

wire composition
PMnCSSi
0.01 %1.65 %0.10 %0.01 %0.30 %

Classifications: ASME SFA 5.17; AWS A5.17; EH12K

x

Typical Weld Metal Analysis %

wire composition
PMnCSSi
0.01 %1.65 %0.10 %0.01 %0.30 %

Classifications: ASME SFA 5.17; AWS A5.17; EH12K

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : SPOOLARC 53
53 5/32X65#CL 1584F34 FIND A DISTRIBUTOR
53 5/32X1000#DR 1586F94 FIND A DISTRIBUTOR
53 1/8X65#CL 1584F32 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..