OK FLUX 429

OK FLUX 429

OK Flux 429 is a neutral, bonded flux intended for butt and fillet welding of carbon and low alloy steel plate. It combines good as welded and stress relieved mechanical properties with excellent performance. Its slag is generally self peeling, even in tight, narrow groove butt welds. It provides moderate tolerance of rust and mill scale. OK Flux 429 is used in offshore oil rig, bridge, ship, pressure vessel, and structural fabrication. It will operate with DC and AC, single and multiwire systems at currents up to 1000 amps.

Where To Buy


Industries

  • Ship and Offshore Yards
  • Bridge Construction
  • Ship/Barge Building
  • Pressure Vessels
  • Process
  • Structural Steel Fabrication
  • Mobile Equipment
  • Power Generation
  • Pipeline
  • Industrial and General Fabrication

Welding Process

  • SAW - Submerged Arc Welding

Specifications


Classifications

AWS - As Welded AWS - PWHT AWS/EN Wire
F9A4-ENi4 Ni4 F8P4-ENi4-ENi4 AWS A5.23: ENi4 Spoolarc ENi4
F7A2-EM12K F6P4-EM12K AWS A5.17: EM12K Spoolarc 81
F8A4-ENi1K-Ni1 - AWS A5.23: ENi1K Spoolarc 75
F7A2-EM14K F7P4-EM14K AWS A5.17: EM14K Spoolarc 71
F7A4-EH12K - AWS A5.17: EH12K Spoolarc 53
F7A2-EM13K - AWS A5.17: EM13K Spoolarc 29S

Typical Mechanical Properties

Charpy V-Notch Charpy V-Notch Testing Temp Condition Elongation Tensile Strength Wire Yield Strength
44 ft-lb -40 °F As Welded 30 % 82 ksi Spoolarc 71 69 ksi
48 ft-lb -20 °F As Welded 26 % 79 ksi Spoolarc 81 66 ksi
38 ft-lb -20 °F As Welded 27 % 83 ksi Spoolarc 29S 67 ksi
30 ft-lb -40 °F As Welded 28 % 85 ksi Spoolarc 53 71 ksi
40 ft-lb -40 °F As Welded 28 % 86 ksi Spoolarc 75 73 ksi
44 ft-lb -40 °F As Welded 25 % 93 ksi Spoolarc ENi4 82 ksi
50 ft-lb -40 °F Stress Relieved 30 % 75 ksi Spoolarc 81 60 ksi
44 ft-lb -20 °F Stress Relieved 32 % 76 ksi Spoolarc 71 63 ksi
24 ft-lb -40 °F Stress Relieved 26 % 89 ksi Spoolarc ENi4 77 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnMoCSSiNi
0.018 %1.50 %0.15 %0.05 %0.012 %0.60 %0.80 %

Approvals: CWB; AWS A5.28 F49A4-ENi1K-Ni1-H8; CWB; CSA W48 F49A3-EM12K (H8)
Classifications: AWS A5.17; F7A2-EM14K; ASME SFA 5.23; ASME SFA 5.17; AWS A5.17; F7A2-EM12K; AWS A5.17; F6P4-EM12K; AWS A5.17; F7A2-EM13K; AWS A5.17; F7P4-EM14K; AWS A5.17; F7A4-EH12K; AWS A5.23; F8A2-EA1-A2; AWS A5.23; F8P2-EA1-A2; AWS A5.23; F8A2-EA2-A3; AWS A5.23; F8P0-EA2-A3; AWS A5.23; F9A4-ENi1K-Ni1; AWS A5.23; F9A4-ENi14-Ni4; AWS A5.23; F8P4-ENi4-Ni4

Approvals are based on factory location. Please contact ESAB for more information.


x

Classifications

AWS - As Welded AWS - PWHT AWS/EN Wire
F9A4-ENi4 Ni4 F8P4-ENi4-ENi4 AWS A5.23: ENi4 Spoolarc ENi4
F7A2-EM12K F6P4-EM12K AWS A5.17: EM12K Spoolarc 81
F8A4-ENi1K-Ni1 - AWS A5.23: ENi1K Spoolarc 75
F7A2-EM14K F7P4-EM14K AWS A5.17: EM14K Spoolarc 71
F7A4-EH12K - AWS A5.17: EH12K Spoolarc 53
F7A2-EM13K - AWS A5.17: EM13K Spoolarc 29S

Typical Mechanical Properties

Charpy V-Notch Charpy V-Notch Testing Temp Condition Elongation Tensile Strength Wire Yield Strength
44 ft-lb -40 °F As Welded 30 % 82 ksi Spoolarc 71 69 ksi
48 ft-lb -20 °F As Welded 26 % 79 ksi Spoolarc 81 66 ksi
38 ft-lb -20 °F As Welded 27 % 83 ksi Spoolarc 29S 67 ksi
30 ft-lb -40 °F As Welded 28 % 85 ksi Spoolarc 53 71 ksi
40 ft-lb -40 °F As Welded 28 % 86 ksi Spoolarc 75 73 ksi
44 ft-lb -40 °F As Welded 25 % 93 ksi Spoolarc ENi4 82 ksi
50 ft-lb -40 °F Stress Relieved 30 % 75 ksi Spoolarc 81 60 ksi
44 ft-lb -20 °F Stress Relieved 32 % 76 ksi Spoolarc 71 63 ksi
24 ft-lb -40 °F Stress Relieved 26 % 89 ksi Spoolarc ENi4 77 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnMoCSSiNi
0.018 %1.50 %0.15 %0.05 %0.012 %0.60 %0.80 %

Approvals: CWB; AWS A5.28 F49A4-ENi1K-Ni1-H8; CWB; CSA W48 F49A3-EM12K (H8)
Classifications: AWS A5.17; F7A2-EM14K; ASME SFA 5.23; ASME SFA 5.17; AWS A5.17; F7A2-EM12K; AWS A5.17; F6P4-EM12K; AWS A5.17; F7A2-EM13K; AWS A5.17; F7P4-EM14K; AWS A5.17; F7A4-EH12K; AWS A5.23; F8A2-EA1-A2; AWS A5.23; F8P2-EA1-A2; AWS A5.23; F8A2-EA2-A3; AWS A5.23; F8P0-EA2-A3; AWS A5.23; F9A4-ENi1K-Ni1; AWS A5.23; F9A4-ENi14-Ni4; AWS A5.23; F8P4-ENi4-Ni4

Approvals are based on factory location. Please contact ESAB for more information.


x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK FLUX 429
OK FLUX 429 50#FLUX PACK 8424FP9 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..