OK FLUX 282

OK FLUX 282

OK Flux 282 is an active, bonded flux designed for high speed, single pass welding of carbon steel sheet. Butt, lap, and fillet welds are well washed and free from undercut even at speeds up to 120 IPM (305 cm/min). It is primarily used with DC single and parallel wire systems at currents up to 1300 amps. OK Flux 282 is recommended for making high speed welds in metallic building beams, spiral pipe, storage tanks, and rail cars. *Single pass application only. Any mechanical property and undiluted weld chemistry listed are for information only.

Where To Buy


Industries

  • Metal Beam Fabrication
  • Pipe Construction
  • Tank and Vessel Fabrication
  • Railcars

Welding Process

  • SAW - Submerged Arc Welding

Specifications


Classifications

AWS - As Welded AWS/EN Wire
F7AZ-EM13K AWS A5.17: EM13K Spoolarc 29S
F7AZ-EM12K AWS A5.17: EM12K Spoolarc 81

Typical Mechanical Properties

Charpy V-Notch Condition Elongation Tensile Strength Wire Yield Strength
14 ft-lb As Welded 22 % 100 ksi Spoolarc 29S 88 ksi
18 ft-lb As Welded 23 % 95 ksi Spoolarc 81 85 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnCSSi
0.03 %1.24 %0.09 %0.02 %0.80 %

Classifications: ASME SFA 5.17; AWS A5.17; F7AZ-EM12K; AWS A5.17; F7AZ-EM13K

x

Classifications

AWS - As Welded AWS/EN Wire
F7AZ-EM13K AWS A5.17: EM13K Spoolarc 29S
F7AZ-EM12K AWS A5.17: EM12K Spoolarc 81

Typical Mechanical Properties

Charpy V-Notch Condition Elongation Tensile Strength Wire Yield Strength
14 ft-lb As Welded 22 % 100 ksi Spoolarc 29S 88 ksi
18 ft-lb As Welded 23 % 95 ksi Spoolarc 81 85 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnCSSi
0.03 %1.24 %0.09 %0.02 %0.80 %

Classifications: ASME SFA 5.17; AWS A5.17; F7AZ-EM12K; AWS A5.17; F7AZ-EM13K

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK FLUX 282
OK FLUX 282 55#BG 8514F09 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..