OK Flux 231 is an active, bonded flux designed for fillet and butt welding of carbon steel plate. It provides excellent tolerance of rust and mill scale so joint preparation can be minimized. This flux will produce horizontal fillets up to 3/8" (9.5 mm) leg size without undercut or rollover. The slag peeling is excellent. OK Flux 231 can be used for multipass welding, but because Mn and Si buildup is possible, welding voltage should be kept to a minimum and plate thickness should be limited to 1" (25 mm). OK Flux 231 is suitable for DC single and parallel wire welding at currents up to 1000 A. It is used for welding rail cars, water heater tanks, ship plates, and structural steel.

BUY NOW


Industries

  • Railcars
  • Tank and Vessel Fabrication
  • Ship/Barge Building
  • Structural Steel Fabrication

Welding Process

  • SAW - Submerged Arc Welding

Specifications


Classifications

AWS - As Welded AWS/EN Wire
F7A2-EM12K AWS A5.17: EM12K Spoolarc 81

Typical Mechanical Properties

Charpy V-Notch Condition Elongation Tensile Strength Wire Yield Strength
28 ft-lb As Welded 27 % 81 ksi Spoolarc 81 67 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnCSSi
0.02 %1.40 %0.08 %0.01 %0.30 %

Approvals: CWB; CSA W48 E49A3-EM12K-H4
Classifications: ASME SFA 5.17; AWS A5.17; F7A2-EM12K; AWS A5.17; F7A2-EL12

Approvals are based on factory location. Please contact ESAB for more information.


x

Classifications

AWS - As Welded AWS/EN Wire
F7A2-EM12K AWS A5.17: EM12K Spoolarc 81

Typical Mechanical Properties

Charpy V-Notch Condition Elongation Tensile Strength Wire Yield Strength
28 ft-lb As Welded 27 % 81 ksi Spoolarc 81 67 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnCSSi
0.02 %1.40 %0.08 %0.01 %0.30 %

Approvals: CWB; CSA W48 E49A3-EM12K-H4
Classifications: ASME SFA 5.17; AWS A5.17; F7A2-EM12K; AWS A5.17; F7A2-EL12

Approvals are based on factory location. Please contact ESAB for more information.


x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK FLUX 231
OK FLUX 231 14X65 55#BG 8334F09 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..