OK Flux 10.62

ESAB

OK Flux 10.62

The following items have been added to your list


x

ESAB OK Flux 10.62 is a high basicity, neutral, bonded flux intended primarily for multipass butt welding carbon and low alloy steel plate. OK Flux 10.62 produces weld metal that is very clean metallurgically and exhibits exceptional impact toughness at low temperatures. OK Flux 10.62 provides well-shaped beads and free peeling slag. Applications for OK Flux 10.62 include offshore oil rigs (meets CTOD requirements), fracture critical bridge members, ship construction, pressure vessels, and tank cars. It is suitable for use with AC and DC, single and multiwire systems at currents up to 1000 amps. OK Flux 10.62 should only be used in applications where the base plate is free of rust and mill scale.

BUY NOW


Welding Process

  • SAW - Submerged Arc Welding

Classifications

Classifications ASME SFA 5.17 :
ASME SFA 5.23 :
AWS A5.17 : F7A8-EM12K
AWS A5.17 : F7P6-EH12K
AWS A5.17 : F6P8-EM12K
AWS A5.17 : F7A6-EM14K
AWS A5.17 : F7P6-EM14K
AWS A5.23 : F8A6-EA2-A2
AWS A5.23 : F9A8-EA3-A3
AWS A5.23 : F9P4-EA3-A3
AWS A5.23 : F7A4-ENi1-Ni1
AWS A5.23 : F8A4-ENi4-Ni4
AWS A5.23 : F8P8-ENi4-Ni4
AWS A5.23 : F8P2-EB2-B2
AWS A5.23 : F8P2-EB3-B3
AWS A5.23 : F9A6-EM2-M2
AWS A5.23 : F11A6-EM4-M4
AWS A5.23 : F12A6-EF5-G
AWS A5.17 : F7A8-EH12K

Approvals

Approvals CE EN 13479
CWB CSA W48 F49A6-EM12K-H8
DB 51.039.07
NAKS/HAKC RD 03-613-03
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Transfer No Silicon or Manganese alloying
Basicity Index nom: 3.2
Density nom: 1.1 kg/dm3
Diffusible Hydrogen max 5 ml H/100g weld metal (Redried flux); max 4 ml H/100g in BlockPac (moisture protection)
Grain Size 0.2-1.6 mm (10x65 mesh)
Slag Type Fluoride-basic

Flux Consumption

Volts kg Flux / kg Wire DC+ kg Flux / kg Wire AC
26 V 0.7 kg 0.6 kg
30 V 1.0 kg 0.9 kg
34 V 1.3 kg 1.2 kg
38 V 1.6 kg 1.4 kg
Amps Dimensions Travel speed
580 A Ø 4.0 mm 55 cm/min

Classifications

Wire AWS/EN AWS - As Welded AWS - PWHT
Spoolarc U515 AWS A5.23: EB2R - F8P2-EB2-B2
Spoolarc ENi4 AWS A5.23: ENi4 F8A4-ENi4-Ni4 F8P8-ENi4-Ni4
Spoolarc 75 AWS A5.23: ENi1K F7A4-ENi1-Ni1
Spoolarc 71 AWS A5.17: EM14K F7A6-EM14K F7P6-EM14K
Spoolarc 53 AWS A5.17: EH12K F7A8-EH12K F7P6-EH12K
Spoolarc 81 AWS A5.17: EM12K F7A8-EM12K F6P8-EM12K, F7P6-EM12K
OK Autrod 13.20 SC AWS A5.23: EB3R - F8P2-EB3-B3

Approvals

Wire ABS BV CE DB DNV GL LR RINA RS VdTÜV
OK Autrod 12.22 * * * * * * * - - *
OK Autrod 12.24 - - * - - - - - - *
OK Autrod 12.32 * * * * * * * * * *
OK Autrod 12.34 * * - - * * * - - -
OK Autrod 13.10 SC - - * * - - - - - *
OK Autrod 13.20 SC - - * - - - - - - *
OK Autrod 13.24 * * * - * * * - - -
OK Autrod 13.27 * * * * * * * * * *
OK Autrod 13.43 * * * - * * * - - -
OK Tubrod 15.27S * - * - * * * - - -
*Selected production units only. Please contact ESAB for more information. Visit esab.com to download specific flux/wire combination fact sheets for more details.

Typical Mechanical Properties

Wire Condition Yield Strength Tensile Strength Charpy V-Notch Elongation
OK Autrod 13.20SC Stress Relieved 1 hr @ 621C (1150F) 530 MPa
(77 ksi)
630 MPa
(91 ksi)
80 J @ -29°C,
(59 ft-lb @ -20 °F)
25 %
Spoolarc 53 As Welded null 485 MPa
(70 ksi)
656 MPa
(82 ksi)
88 J @ -62°C,
(65 ft-lb @ -80 °F)
29 %
Spoolarc 53 Stress Relieved 1 hr @ 621C (1150F) 430 MPa
(63 ksi)
530 MPa
(77 ksi)
114 J @ -51°C,
(84 ft-lb @ -60 °F)
31 %
Spoolarc 71 As Welded null 515 MPa
(75 ksi)
590 MPa
(85 ksi)
136 J @ -51°C,
(100 ft-lb @ -60 °F)
28 %
Spoolarc 71 Stress Relieved 1 hr @ 621C (1150F) 500 MPa
(72 ksi)
575 MPa
(83 ksi)
160 J @ -51°C,
(119 ft-lb @ -60 °F)
30 %
Spoolarc 71 Stress Relieved 8 hrs @ 621C (1150F) 515 MPa
(74 ksi)
570 MPa
(83 ksi)
187 J @ -51°C,
(138 ft-lb @ -60 °F)
28 %
Spoolarc 75 As Welded null 475 MPa
(69 ksi)
550 MPa
(80 ksi)
136 J @ -40°C,
(100 ft-lb @ -40 °F)
60 %
Spoolarc 81 As Welded null 450 MPa
(65 ksi)
555 MPa
(75 ksi)
150 J @ -51°C,
(110 ft-lb @ -60 °F)
32 %
Spoolarc 81 Stress Relieved 1 hr @ 621C (1150F) 370 MPa
(54 ksi)
480 MPa
(70 ksi)
217 J @ -46°C,
(160 ft-lb @ -50 °F)
32 %
Spoolarc ENi4 As Welded null 510 MPa
(74 ksi)
595 MPa
(86 ksi)
132 J @ -40°C,
(97 ft-lb @ -40 °F)
29 %
Spoolarc ENi4 Stress Relieved 1 hr @ 621C (1150F) 515 MPa
(75 ksi)
610 MPa
(89 ksi)
64 J @ -73°C,
(47 ft-lb @ -100 °F)
28 %
Spoolarc ENi4 Stress Relieved 8 hrs @ 621C (1150F) 540 MPa
(78 ksi)
645 MPa
(90 ksi)
84 J @ -73°C,
(62 ft-lb @ -100 °F)
27 %
Spoolarc U515 Stress Relieved 1 hr @ 621C (1150F) 515 MPa
(75 ksi)
600 MPa
(87 ksi)
190 J @ -29°C,
(140 ft-lb @ -20 °F)
27 %
Spoolarc U515 Stress Relieved 8 hrs @ 621C (1150F) 515 MPa
(75 ksi)
600 MPa
(87 ksi)
190 J @ -29°C,
(140 ft-lb @ -20 °F)
27 %

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Mn Mo Ni P S Si
OK Autrod 13.20SC
0.08 % 2.0 % 0.85 % 0.60 % 0.85 % - 0.010 % 0.005 % 0.20 %
Spoolarc 53
0.08 % - - 1.5 % - - 0.018 % 0.009 % 0.3 %
Spoolarc 71
0.06 % - - 1.1 % - - 0.012 % 0.004 % 0.4 %
Spoolarc 75
0.07 % - - 1.0 % - 0.8 % 0.009 % 0.005 % 0.5 %
Spoolarc 81
0.07 % - - 1.0 % - - 0.016 % 0.007 % 0.3 %
Spoolarc ENi4
0.01 % - - 1.8 % 0.16 % 1.8 % 0.004 % 0.004 % 0.3 %
Spoolarc U515
0.05 % 1.60 % 0.52 % 0.70 % 0.52 % 0.04 % 0.011 % 0.007 % 0.19 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Flux 10.62
OK Flux 10.62 1000kg(2200lb) 1062H00N00 FIND A DISTRIBUTOR
OK Flux 10.62 1000kg(2200lb) 1U62H02000 FIND A DISTRIBUTOR
OK Flux 10.62 25kg(55lb) BP 1U62802000 FIND A DISTRIBUTOR
OK Flux 10.62 900kg(1980lb) 1062G00000 FIND A DISTRIBUTOR
x
x

x

Loading..