Spoolarc ENi4

The following items have been added to your list


x

Designed for single or multipass welding on high strength steels. Produces good low temperature toughness on a variety of base materials. Weld metal tensile strengths are in excess of 90 ksi (620 MPa) in both the as welded and stress relieved conditions. Applications include pressure vessels, offshore oil rigs, bridges, and other structural steel fabrication.

BUY NOW


Industries

  • Bridge Construction
  • Offshore Oil
  • Pressure Vessels
  • Structural Steel Fabrication

Welding Process

  • SAW - Submerged Arc Welding

Classifications

Classifications ASME SFA 5.23 :
AWS A5.23 : ENi4

Approvals

Grade AWS A5.23: ENi4
Society ABS
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cu Mn Mo Ni P S Si
0.17 % 0.06 % 0.73 % 0.17 % 1.74 % 0.00 % 0.00 % 0.19 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Spoolarc ENi4
2214F32 Find a distributor
2216F50 Find a distributor
2214F30 Find a distributor
2214F30CB Find a distributor
2214L30 Find a distributor
2216F54 Find a distributor
2214F34 Find a distributor
2214F29CB Find a distributor

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..