Spoolarc 75 is a copper-coated 1% nickel solid wire for carbon steel and low alloy welding applications using Submerged Arc Welding (SAW) processes. Spoolarc 75 produces a deposit that meets the weathering requirements of AWS D1.1 and D1.5 and is designed to weld weathering steels and/or where improved low temperature impact toughness is specified. Spoolarc 75 is typically used with a neutral flux such as ESAB OK Flux 429, 10.71, and 10.62. Spoolarc 75 is used for bridge and structural welding.

BUY NOW


Industries

  • Bridge Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Ship/Barge Building

Welding Process

  • SAW - Submerged Arc Welding

Classifications

Classifications ASME SFA 5.23 :
AWS A5.23 : ENi1K

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Cu Mn Mo Ni P S Si
0.08 % 0.04 % 0.07 % 0.89 % 0.01 % 0.98 % 0.00 % 0.01 % 0.46 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Spoolarc 75
13P2F05 Find a distributor
13P2F07 Find a distributor

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..