Cr-, Mo-alloyed, copper-coated wire for Submerged Arc Welding. Very low level of impurities. X-bar (Bruscato-) max. 7. With OK Flux 10.65 for highest toughness requirements also after Step-Cooling; very clean weld metal with X-bar max. 10. Mainly for creep resistant steels (2,25% Cr, 1% Mo).

BUY NOW


Classifications

Wire Electrode SFA/AWS A5.23 : EB3R
EN ISO 24598-A : S S CrMo2

Approvals

Grade EN 13479
Society CE
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Wire Composition %
Al As B C Cr Cu J-Factor Mn Mn+Si Mo Nb Nb+Ti+V Ni P P+Sn S Sb Si Sn Ti V X-bar
0.005 % 0.003 % 0.0005 % 0.11 % 2.50 % 0.08 % 50 % 0.65 % 0.75 % 1.00 % 0.006 % 0.014 % 0.08 % 0.003 % 0.006 % 0.003 % 0.002 % 0.10 % 0.003 % 0.002 % 0.006 % 5 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod B3 SC
13S3252800 FIND A DISTRIBUTOR
13S3320400 FIND A DISTRIBUTOR
13S3322800 FIND A DISTRIBUTOR
13S3400400 FIND A DISTRIBUTOR
13S3402800 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..