OK Autrod 13.20SC is a Cr-, Mo-alloyed, copper-coated wire for Submerged Arc Welding. Very low level of impurities. X-factor (Bruscato-) max. 11. With OK Flux 10.63 for highest toughness requirements also after Step-Cooling; very clean weld metal with X-factor max. 15. Mainly for creep resistant steels (2,25% Cr, 1% Mo).

BUY NOW


Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn Mo P S Si
0.10 % 2.30 % 0.63 % 1.00 % 0.01 % 0.004 % 0.16 %

Approvals

Society CE
Grade EN 13479
Approvals are based on factory location. Please contact ESAB for more information.

Classifications

Name SFA/AWS A5.23
Grade EB3R
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 13.20 SC
OK Autrod 13.20 SC 2.0mm 30kg 132S202800 FIND A DISTRIBUTOR
OK AUTROD 13.20SC 2.5MM 30KGCL 132S252800 FIND A DISTRIBUTOR
OK Autrod 13.20 SC 3.0mm 280kg 132S300400 FIND A DISTRIBUTOR
OK Autrod 13.20 SC 3.0mm 30kg 132S302800 FIND A DISTRIBUTOR
OK AUTROD 13.20SC 3.2MM 30KGCL 132S322800 FIND A DISTRIBUTOR
OK Autrod 13.20 SC 4.0mm 280kg 132S400400 FIND A DISTRIBUTOR
OK AUTROD 13.20SC 4.0MM 30KGCL 132S402800 FIND A DISTRIBUTOR
x
x

x

Loading..